<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Da Vinci 1.0 Pro filament size]]></title>
		<link>https://www.soliforum.com/topic/17135/da-vinci-10-pro-filament-size/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/17135/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Da Vinci 1.0 Pro filament size.]]></description>
		<lastBuildDate>Wed, 14 Feb 2018 00:19:47 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Da Vinci 1.0 Pro filament size]]></title>
			<link>https://www.soliforum.com/post/142507/#p142507</link>
			<description><![CDATA[<div class="quotebox"><cite>parkerclan22 wrote:</cite><blockquote><p>so i accidentally ordered 3mm (2.85mm) PETG filament.....my question is, can i extrude this through this printer?&nbsp; &nbsp;its completely stock, but i use Simplify3d so i can control feedrates quite well.&nbsp; I know it will likely be slower, but i typically print ABS and PLA slower than most would.</p></blockquote></div><p>It&#039;s 1.75mm only. In fact there are very few printers on the market anymore that use the 3mm stuff. So you would be better off trying to get a return. The 3mm stuff will not fit the throat of the extruder.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Wed, 14 Feb 2018 00:19:47 +0000</pubDate>
			<guid>https://www.soliforum.com/post/142507/#p142507</guid>
		</item>
		<item>
			<title><![CDATA[Da Vinci 1.0 Pro filament size]]></title>
			<link>https://www.soliforum.com/post/142506/#p142506</link>
			<description><![CDATA[<p>so i accidentally ordered 3mm (2.85mm) PETG filament.....my question is, can i extrude this through this printer?&nbsp; &nbsp;its completely stock, but i use Simplify3d so i can control feedrates quite well.&nbsp; I know it will likely be slower, but i typically print ABS and PLA slower than most would.</p>]]></description>
			<author><![CDATA[null@example.com (parkerclan22)]]></author>
			<pubDate>Wed, 14 Feb 2018 00:08:55 +0000</pubDate>
			<guid>https://www.soliforum.com/post/142506/#p142506</guid>
		</item>
	</channel>
</rss>