<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Take apart extruder housing]]></title>
		<link>https://www.soliforum.com/topic/16707/take-apart-extruder-housing/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/16707/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Take apart extruder housing.]]></description>
		<lastBuildDate>Sat, 09 Sep 2017 21:00:21 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Take apart extruder housing]]></title>
			<link>https://www.soliforum.com/post/137888/#p137888</link>
			<description><![CDATA[<p>Da vinci Jr.? take out four screws from fan, remove fan, take out two screws under the fan, then try to push the little tabs in on the side with a small screwdriver and gently pry the top up.</p>]]></description>
			<author><![CDATA[null@example.com (yizhou.he)]]></author>
			<pubDate>Sat, 09 Sep 2017 21:00:21 +0000</pubDate>
			<guid>https://www.soliforum.com/post/137888/#p137888</guid>
		</item>
		<item>
			<title><![CDATA[Re: Take apart extruder housing]]></title>
			<link>https://www.soliforum.com/post/137672/#p137672</link>
			<description><![CDATA[<p>I you carefully push the little tabs in on the side with a small screwdriver and gently pry the top up. When you get one side up the other side should come off without to much effort. DON&#039;T FORCE IT!</p>]]></description>
			<author><![CDATA[null@example.com (Bozotclown1970)]]></author>
			<pubDate>Sat, 02 Sep 2017 23:50:30 +0000</pubDate>
			<guid>https://www.soliforum.com/post/137672/#p137672</guid>
		</item>
		<item>
			<title><![CDATA[Take apart extruder housing]]></title>
			<link>https://www.soliforum.com/post/137671/#p137671</link>
			<description><![CDATA[<p>While removing the filament feeder tube, I unscrewed the metal fitting, leaving part of it inside the extruder housing.&nbsp; How can I open the extruder box, so I can reassemble the filament input set up?</p>]]></description>
			<author><![CDATA[null@example.com (rfriedma)]]></author>
			<pubDate>Sat, 02 Sep 2017 23:10:54 +0000</pubDate>
			<guid>https://www.soliforum.com/post/137671/#p137671</guid>