<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — problem on wearing metal]]></title>
		<link>https://www.soliforum.com/topic/16378/problem-on-wearing-metal/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/16378/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in problem on wearing metal.]]></description>
		<lastBuildDate>Tue, 25 Apr 2017 08:17:18 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: problem on wearing metal]]></title>
			<link>https://www.soliforum.com/post/134884/#p134884</link>
			<description><![CDATA[<p>just added my included filter. thanks, elmore!</p>]]></description>
			<author><![CDATA[null@example.com (frostmoore)]]></author>
			<pubDate>Tue, 25 Apr 2017 08:17:18 +0000</pubDate>
			<guid>https://www.soliforum.com/post/134884/#p134884</guid>
		</item>
		<item>
			<title><![CDATA[Re: problem on wearing metal]]></title>
			<link>https://www.soliforum.com/post/134862/#p134862</link>
			<description><![CDATA[<p>There will always be some wear in any extruder (even industrial ones), this is why the melt filter nozzle was created, to filter out contaminants.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Mon, 24 Apr 2017 16:26:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/134862/#p134862</guid>
		</item>
		<item>
			<title><![CDATA[problem on wearing metal]]></title>
			<link>https://www.soliforum.com/post/134850/#p134850</link>
			<description><![CDATA[<p>just as said on title. </p><p>my filastruder keep producing filaments with metal bits and black powders. </p><p>i spent whole month flushing filastruder with various materials (PLA, PCL, ABS which provided) and this is not solved.</p><p>i need help very much.&nbsp; any suggestion?</p>]]></description>
			<author><![CDATA[null@example.com (frostmoore)]]></author>
			<pubDate>Mon, 24 Apr 2017 09:37:06 +0000</pubDate>
			<guid>https://www.soliforum.com/post/134850/#p134850</guid>