<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — High temp silicone]]></title>
		<link>https://www.soliforum.com/topic/16317/high-temp-silicone/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/16317/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in High temp silicone.]]></description>
		<lastBuildDate>Sat, 08 Apr 2017 01:58:51 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: High temp silicone]]></title>
			<link>https://www.soliforum.com/post/134384/#p134384</link>
			<description><![CDATA[<div class="quotebox"><cite>Tin Falcon wrote:</cite><blockquote><p>There is also this stuff&nbsp; good to&nbsp; 1095c&nbsp; &nbsp;<a href="http://www.acehardware.com/product/index.jsp?productId=1445565&amp;KPID=1245588&amp;cid=CAPLA:G:Shopping_-_Cements_-_New&amp;pla=pla_1245588&amp;k_clickid=dce62dbf-8d67-4c8d-965e-5de1fcd2ae8c">http://www.acehardware.com/product/inde … e1fcd2ae8c</a></p><p><span class="postimg"><img src="http://www.acehardware.com/product/http%3A//ace.imageg.net/graphics/product_images/pACE3-1245588enh-z6.jpg" alt="http://www.acehardware.com/product/http%3A//ace.imageg.net/graphics/product_images/pACE3-1245588enh-z6.jpg" /></span><br />hmm</p></blockquote></div><p>In case you need to repair a hole in your rocket engine..</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Sat, 08 Apr 2017 01:58:51 +0000</pubDate>
			<guid>https://www.soliforum.com/post/134384/#p134384</guid>
		</item>
		<item>
			<title><![CDATA[Re: High temp silicone]]></title>
			<link>https://www.soliforum.com/post/134382/#p134382</link>
			<description><![CDATA[<p>There is also this stuff&nbsp; good to&nbsp; 1095c&nbsp; &nbsp;<a href="http://www.acehardware.com/product/index.jsp?productId=1445565&amp;KPID=1245588&amp;cid=CAPLA:G:Shopping_-_Cements_-_New&amp;pla=pla_1245588&amp;k_clickid=dce62dbf-8d67-4c8d-965e-5de1fcd2ae8c">http://www.acehardware.com/product/inde … e1fcd2ae8c</a></p><p><span class="postimg"><img src="http://www.acehardware.com/product/http%3A//ace.imageg.net/graphics/product_images/pACE3-1245588enh-z6.jpg" alt="http://www.acehardware.com/product/http%3A//ace.imageg.net/graphics/product_images/pACE3-1245588enh-z6.jpg" /></span><br />hmm</p>]]></description>
			<author><![CDATA[null@example.com (Tin Falcon)]]></author>
			<pubDate>Sat, 08 Apr 2017 00:00:42 +0000</pubDate>
			<guid>https://www.soliforum.com/post/134382/#p134382</guid>
		</item>
		<item>
			<title><![CDATA[Re: High temp silicone]]></title>
			<link>https://www.soliforum.com/post/134372/#p134372</link>
			<description><![CDATA[<p>They make one for the automotive industry that is good to 800F but it has copper in it so it would only be good for things like taking a silicone heater to a bed or something similar.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Thu, 06 Apr 2017 23:28:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/134372/#p134372</guid>
		</item>
		<item>
			<title><![CDATA[High temp silicone]]></title>
			<link>https://www.soliforum.com/post/134370/#p134370</link>
			<description><![CDATA[<p>today at the local hardware store picked up a tube of this</p><p><a href="http://www.acehardware.com/product/index.jsp?productId=1445567&amp;KPID=1245596&amp;cid=CAPLA:G:Shopping_-_Cements&amp;pla=pla_1245596&amp;k_clickid=dce62dbf-8d67-4c8d-965e-5de1fcd2ae8c">http://www.acehardware.com/product/inde … e1fcd2ae8c</a></p><p>Seems like the red has a 20% higher heat rating&nbsp; 600f instead of 500 so better around hot ends but this should work just fine for holding wires on the heat bed and insulating bare connectors.</p>]]></description>
			<author><![CDATA[null@example.com (Tin Falcon)]]></author>