<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Filastruder Speed Control]]></title>
		<link>https://www.soliforum.com/topic/16130/filastruder-speed-control/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/16130/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Filastruder Speed Control.]]></description>
		<lastBuildDate>Sat, 11 Feb 2017 15:52:49 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Filastruder Speed Control]]></title>
			<link>https://www.soliforum.com/post/132407/#p132407</link>
			<description><![CDATA[<p>Yes. Instructions for CC are in the main assembly instructions document.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 11 Feb 2017 15:52:49 +0000</pubDate>
			<guid>https://www.soliforum.com/post/132407/#p132407</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder Speed Control]]></title>
			<link>https://www.soliforum.com/post/132403/#p132403</link>
			<description><![CDATA[<p>Thank you elmoret. Is the CV adjustment the top left small screw? Also, where can I find the instructions for the CC adjustment?</p>]]></description>
			<author><![CDATA[null@example.com (aliowaisanwer)]]></author>
			<pubDate>Sat, 11 Feb 2017 13:38:06 +0000</pubDate>
			<guid>https://www.soliforum.com/post/132403/#p132403</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder Speed Control]]></title>
			<link>https://www.soliforum.com/post/132352/#p132352</link>
			<description><![CDATA[<p>The CV adjustment reduces the speed. It is a multi turn potentiometer, it may take a dozen or so rotations to get into the range needed to reduce the voltage. Counter-clockwise reduces voltage.</p><p>The CC adjustment needs to be set as detailed in the instructions. It is important this is set properly or damage to the machine may result.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Fri, 10 Feb 2017 06:34:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/132352/#p132352</guid>
		</item>
		<item>
			<title><![CDATA[Filastruder Speed Control]]></title>
			<link>https://www.soliforum.com/post/132350/#p132350</link>
			<description><![CDATA[<p>Hi,</p><p>I would like to control the speed of the filastruder. I tried loosening/tightening both the tiny screws ontop of the display at the back, nbut it seems to have no effect. Please help me on how to control the speed.</p><p>Thank you</p>]]></description>
			<author><![CDATA[null@example.com (aliowaisanwer)]]></author>