<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — davinci 1.0a with repetier print issues]]></title>
		<link>https://www.soliforum.com/topic/16001/davinci-10a-with-repetier-print-issues/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/16001/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in davinci 1.0a with repetier print issues.]]></description>
		<lastBuildDate>Tue, 10 Jan 2017 07:00:30 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: davinci 1.0a with repetier print issues]]></title>
			<link>https://www.soliforum.com/post/130851/#p130851</link>
			<description><![CDATA[<p>no i didn&#039;t do that. actually didn&#039;t know i had to do that thanks. ill give it a try and see how it dose.</p>]]></description>
			<author><![CDATA[null@example.com (shaggy)]]></author>
			<pubDate>Tue, 10 Jan 2017 07:00:30 +0000</pubDate>
			<guid>https://www.soliforum.com/post/130851/#p130851</guid>
		</item>
		<item>
			<title><![CDATA[Re: davinci 1.0a with repetier print issues]]></title>
			<link>https://www.soliforum.com/post/130789/#p130789</link>
			<description><![CDATA[<p>Could be under extrusion. Did you measure the diameter of the filament and set your slicer accordingly? Every roll will be different and the printer must be recalibrated with every roll change and type of material.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Mon, 09 Jan 2017 12:26:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/130789/#p130789</guid>
		</item>
		<item>
			<title><![CDATA[davinci 1.0a with repetier print issues]]></title>
			<link>https://www.soliforum.com/post/130775/#p130775</link>
			<description><![CDATA[<p>hey everyone im having issues printing abs with repetier on my flashed davinci 1.0a. ( photos for reference) as you can tell im having some odd layer shrinkage that is making my prints come out really bad. im not sure how to adjust the printer to fix this issue. any help would be awesome. i am using slic3r as my slicing software</p>]]></description>