<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Extruder gets clogged constantly, help please]]></title>
		<link>https://www.soliforum.com/topic/15820/extruder-gets-clogged-constantly-help-please/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/15820/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Extruder gets clogged constantly, help please.]]></description>
		<lastBuildDate>Sat, 10 Dec 2016 15:53:09 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Extruder gets clogged constantly, help please]]></title>
			<link>https://www.soliforum.com/post/128994/#p128994</link>
			<description><![CDATA[<p>Well i think the problme is solved, i clenaed the entire hotend (again) and tightened strong and now it works fine.<br /> Thank you so much for you answers!!!!!</p>]]></description>
			<author><![CDATA[null@example.com (umurtumer10)]]></author>
			<pubDate>Sat, 10 Dec 2016 15:53:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128994/#p128994</guid>
		</item>
		<item>
			<title><![CDATA[Re: Extruder gets clogged constantly, help please]]></title>
			<link>https://www.soliforum.com/post/128944/#p128944</link>
			<description><![CDATA[<p>Is comming out of every hole, the resistor hole, the thermistor hole over the heater block and over the noozle</p>]]></description>
			<author><![CDATA[null@example.com (umurtumer10)]]></author>
			<pubDate>Fri, 09 Dec 2016 21:19:24 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128944/#p128944</guid>
		</item>
		<item>
			<title><![CDATA[Re: Extruder gets clogged constantly, help please]]></title>
			<link>https://www.soliforum.com/post/128943/#p128943</link>
			<description><![CDATA[<p>Is the plastic coming out of the top or bottom of the heater block?</p>]]></description>
			<author><![CDATA[null@example.com (widespreaddeadhead)]]></author>
			<pubDate>Fri, 09 Dec 2016 21:01:55 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128943/#p128943</guid>
		</item>
		<item>
			<title><![CDATA[Re: Extruder gets clogged constantly, help please]]></title>
			<link>https://www.soliforum.com/post/128934/#p128934</link>
			<description><![CDATA[<p>the overflow is getting worse and now the plastic is getting inside the thermistor hole and cheats the readings any siggestion what this could be?</p>]]></description>
			<author><![CDATA[null@example.com (umurtumer10)]]></author>
			<pubDate>Fri, 09 Dec 2016 15:44:14 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128934/#p128934</guid>
		</item>
		<item>
			<title><![CDATA[Re: Extruder gets clogged constantly, help please]]></title>
			<link>https://www.soliforum.com/post/128922/#p128922</link>
			<description><![CDATA[<p>ok so here is the thing i chanched the thermistor to see if the temp is correct and with the other thermistor the temp marked is 165 degrees when i set it to 190 in pronterface, because of that i raise it to 220 in pronterface and the thermistor marks 190 the fan on and it seeems to print but it overflows everywhere i ve attached a video but the quiality is very poor sorry for that</p><p><a href="https://youtu.be/wEIJ4KAi_0I">https://youtu.be/wEIJ4KAi_0I</a></p><p>any suggestions for the oveflow?</p>]]></description>
			<author><![CDATA[null@example.com (umurtumer10)]]></author>
			<pubDate>Fri, 09 Dec 2016 12:55:03 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128922/#p128922</guid>
		</item>
		<item>
			<title><![CDATA[Re: Extruder gets clogged constantly, help please]]></title>
			<link>https://www.soliforum.com/post/128920/#p128920</link>
			<description><![CDATA[<p>Thank for the answer. The acetone does not disolve the PLA but its easier to remove after a couple of hours in acetone. I use the acetone to soften the PLA and it works pretty well, i remove remains with torch ass yo say. The brand of the PLA is fillamentum 2.85mm and i ve changed to higher temps but still clogging. I have not tried different brand because it worked very good with te first pieces and now just don t. And that is what i can not undertand.</p>]]></description>
			<author><![CDATA[null@example.com (umurtumer10)]]></author>
			<pubDate>Fri, 09 Dec 2016 12:38:02 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128920/#p128920</guid>
		</item>
		<item>
			<title><![CDATA[Re: Extruder gets clogged constantly, help please]]></title>
			<link>https://www.soliforum.com/post/128919/#p128919</link>
			<description><![CDATA[<p>PLA cannot be dissolved by acetone.&nbsp; It only works for&nbsp; ABS. The people that did have clogs usually burned it out using a torch on the metal parts only.&nbsp; You can also try to master the cold pull method but good luck on that. Google it for more info. What brand filament are you using?&nbsp; Have you tried higher temps. Have you tried a different brand?</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Fri, 09 Dec 2016 12:25:18 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128919/#p128919</guid>
		</item>
		<item>
			<title><![CDATA[Extruder gets clogged constantly, help please]]></title>
			<link>https://www.soliforum.com/post/128918/#p128918</link>
			<description><![CDATA[<p>Hello everyone i ve got a really anoying problem and i just dont know what else to do. I ve got a prusa i3 and printed successfull 10 pieces aprox. and any problem untill a couple of days ago, the extruder gets clogged constantly y can t print anything at all. The parts i printed so far were printed with PLA, 190 degrees with the fan in automatic using Slic3r. I ve dismantle the entire Hotend twice and gave the parts an acetone bath for two nights but nothing, it stills heting jammed. I would apreciate the help so much. If you need any detail feel freeto ask.</p><p>thanks</p>]]></description>
			<author><![CDATA[null@example.com (umurtumer10)]]></author>
			<pubDate>Fri, 09 Dec 2016 11:43:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128918/#p128918</guid>
		</item>
	</channel>