<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — print problem]]></title>
		<link>https://www.soliforum.com/topic/15743/print-problem/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/15743/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in print problem.]]></description>
		<lastBuildDate>Tue, 22 Nov 2016 20:07:29 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: print problem]]></title>
			<link>https://www.soliforum.com/post/128268/#p128268</link>
			<description><![CDATA[<p>Hi Pete, </p><p>Many people have their own preferred way of drying filament. </p><p>Leaving your rolls of filament in an air tight container with some silica gel is a good way to store filament. This may take the moisture out over time. </p><p>You can use an oven at around 60 or 70degrees to dry out your spools. However, be careful as PLA starts to soften at only a tiny bit above these temperatures so don&#039;t go too hot with the oven otherwise you&#039;ll just end up with a clump of plastic. </p><p>If you have a boiler for your central heating you can leave it on top of that for a while?</p><p>I hope this helps, <br />Regards,<br /><a href="http://www.3dexfilament.co.uk">www.3dexfilament.co.uk</a> - Black Friday Sales Now On</p>]]></description>
			<author><![CDATA[null@example.com (3Dex)]]></author>
			<pubDate>Tue, 22 Nov 2016 20:07:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128268/#p128268</guid>
		</item>
		<item>
			<title><![CDATA[Re: print problem]]></title>
			<link>https://www.soliforum.com/post/128245/#p128245</link>
			<description><![CDATA[<p>Thanks guys. Changed rolls and nozzle and problem went away. Another thing learned about PLA <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /><br />How can I safely dry the filament as I have over 3/4 kg left on the roll and don&#039;t want to waste it<br />Pete</p>]]></description>
			<author><![CDATA[null@example.com (Pete49)]]></author>
			<pubDate>Mon, 21 Nov 2016 04:36:21 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128245/#p128245</guid>
		</item>
		<item>
			<title><![CDATA[Re: print problem]]></title>
			<link>https://www.soliforum.com/post/128241/#p128241</link>
			<description><![CDATA[<p>moisture and/or a partial clog</p>]]></description>
			<author><![CDATA[null@example.com (heartless)]]></author>
			<pubDate>Mon, 21 Nov 2016 02:05:33 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128241/#p128241</guid>
		</item>
		<item>
			<title><![CDATA[Re: print problem]]></title>
			<link>https://www.soliforum.com/post/128225/#p128225</link>
			<description><![CDATA[<p>How old is this filament and how long has it been in the open air. It looks like moisture to me.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Sun, 20 Nov 2016 04:31:41 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128225/#p128225</guid>
		</item>
		<item>
			<title><![CDATA[Re: print problem]]></title>
			<link>https://www.soliforum.com/post/128224/#p128224</link>
			<description><![CDATA[<p>What is all the discoloration in the print?&nbsp; Do you extrude your own PLA?&nbsp; I assume you are printing in white.&nbsp; It looks like dirty snow.&nbsp; I really can&#039;t see what your problem is.&nbsp; Someone with a little more expertise will chime in soon.&nbsp; I&#039;ll keep an eye on this thread, maybe I can learn somethin......</p><p>Ski</p>]]></description>
			<author><![CDATA[null@example.com (Ski52)]]></author>
			<pubDate>Sun, 20 Nov 2016 03:46:11 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128224/#p128224</guid>
		</item>
		<item>
			<title><![CDATA[print problem]]></title>
			<link>https://www.soliforum.com/post/128223/#p128223</link>
			<description><![CDATA[<p>My kit printer has been working well until last night when this print turned out too thin(?) Any ideas as to a fix?<br />I didn&#039;t change any settings and have not had a power failure so can&#039;t work out what happened or how to repair the problem. I have attached a pic to show the problem. Its PLA filament and<br />it hasn&#039;t been a problem before.<br />Pete</p>]]></description>