<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
		<link>https://www.soliforum.com/topic/15586/perfect-printing-surface-prints-never-stick-when-finished-20/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/15586/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in "Perfect" Printing surface. Prints never stick when finished. $20.]]></description>
		<lastBuildDate>Thu, 12 Oct 2017 10:24:15 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/138832/#p138832</link>
			<description><![CDATA[<p>glass or a tshirt works just fine for me</p>]]></description>
			<author><![CDATA[null@example.com (Kronikabuse)]]></author>
			<pubDate>Thu, 12 Oct 2017 10:24:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/138832/#p138832</guid>
		</item>
		<item>
			<title><![CDATA[Re: "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/138830/#p138830</link>
			<description><![CDATA[<p>What I understand about perfect printing is when you get your desired colour, logo, size or shape of a printed item.<br />and one of the usual that I used is a custom sticker for my little business as well as my business cards.<br />the webpage was <a href="http://www.stickermarket.co.uk">www.stickermarket.co.uk</a>&nbsp; and it works for me.</p>]]></description>
			<author><![CDATA[null@example.com (amandahlauridsen22)]]></author>
			<pubDate>Thu, 12 Oct 2017 06:18:43 +0000</pubDate>
			<guid>https://www.soliforum.com/post/138830/#p138830</guid>
		</item>
		<item>
			<title><![CDATA[Re: "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/127467/#p127467</link>
			<description><![CDATA[<p>Letting it cool to take the print off in order to start another is a waste of time!&nbsp; I have at least 2 pieces of window glass sprayed and ready.&nbsp; I don&#039;t &#039;glue&#039; them to the bed with hairspray, I use 2 clips.&nbsp; Immediately following the finish of a print I remove the hot glass with the print on it and replace it with another piece - continue to print.&nbsp; Takes maybe a minute.&nbsp; Then I can deal with removing the print. <br />Takes me just under 3 min to get to 97C from cold and 10 to 12 to return to cold.&nbsp; Hairspray &amp; glass and I have to use a razor scraper to remove either ABS or PLA - usually no warping.&nbsp; <br />Waste of 20.00 <br />My 0.02</p>]]></description>
			<author><![CDATA[null@example.com (Ski52)]]></author>
			<pubDate>Mon, 10 Oct 2016 03:45:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/127467/#p127467</guid>
		</item>
		<item>
			<title><![CDATA[Re: "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/127437/#p127437</link>
			<description><![CDATA[<p>Hairspray and/or ABS juice works for me as well on a removable glass sheet. If anything is stuck on too hard to remove, taking off the glass and popping it in the freezer for a few minutes always works (I usually hear a terrifying &quot;crack!&quot; from inside the freezer, but when I look, both the print and the glass are in perfect condition, and have separated cleanly).</p>]]></description>
			<author><![CDATA[null@example.com (Claghorn)]]></author>
			<pubDate>Sun, 09 Oct 2016 13:12:41 +0000</pubDate>
			<guid>https://www.soliforum.com/post/127437/#p127437</guid>
		</item>
		<item>
			<title><![CDATA[Re: "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/127412/#p127412</link>
			<description><![CDATA[<p>I used to remove the glass before applying hairspray but lately it has been working just fine by spraying some on a paper towel and wiping the glass with it. It is much easier since a few of my printers have been fitted with a leveling system very similar to the Lulzbot Taz mini.</p>]]></description>
			<author><![CDATA[null@example.com (Revolve3D)]]></author>
			<pubDate>Sat, 08 Oct 2016 16:31:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/127412/#p127412</guid>
		</item>
		<item>
			<title><![CDATA[Re: "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/127405/#p127405</link>
			<description><![CDATA[<p>Shut off your little fans before you spray it. Watch that you don&#039;t get it on your filament or proximity sensor (if you have one) or your slides or belts. It will sure gum things up. When I used hair spray I would remove the mirror (from the bed), wash and dry it, spray it, then return it to the printer. But yeah, it works. Just not as clean as PEI or one of the new made to order surfaces.</p>]]></description>
			<author><![CDATA[null@example.com (Heartlander)]]></author>
			<pubDate>Sat, 08 Oct 2016 14:44:24 +0000</pubDate>
			<guid>https://www.soliforum.com/post/127405/#p127405</guid>
		</item>
		<item>
			<title><![CDATA[Re: "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/127403/#p127403</link>
			<description><![CDATA[<div class="quotebox"><cite>carl_m1968 wrote:</cite><blockquote><p>Hairspray works the same for me,&nbsp; costs 2 bucks and last for a half year at my usage.</p></blockquote></div><p>Yup, same here... <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></description>
			<author><![CDATA[null@example.com (heartless)]]></author>
			<pubDate>Sat, 08 Oct 2016 12:53:08 +0000</pubDate>
			<guid>https://www.soliforum.com/post/127403/#p127403</guid>
		</item>
		<item>
			<title><![CDATA[Re: "Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/127395/#p127395</link>
			<description><![CDATA[<p>Hairspray works the same for me,&nbsp; costs 2 bucks and last for a half year at my usage.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Sat, 08 Oct 2016 00:36:27 +0000</pubDate>
			<guid>https://www.soliforum.com/post/127395/#p127395</guid>
		</item>
		<item>
			<title><![CDATA["Perfect" Printing surface. Prints never stick when finished. $20]]></title>
			<link>https://www.soliforum.com/post/127394/#p127394</link>
			<description><![CDATA[<p><a href="http://www.3ders.org/articles/20161007-3m-japan-fights-warping-and-3d-print-removal-problems-with-special-polyester-print-bed-sheet.html">http://www.3ders.org/articles/20161007- … sheet.html</a></p>]]></description>
			<author><![CDATA[null@example.com (Heartlander)]]></author>