<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — How to get a matte finish on ABS after acetone vapor bath?]]></title>
		<link>https://www.soliforum.com/topic/14777/how-to-get-a-matte-finish-on-abs-after-acetone-vapor-bath/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/14777/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in How to get a matte finish on ABS after acetone vapor bath?.]]></description>
		<lastBuildDate>Thu, 12 May 2016 12:33:06 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: How to get a matte finish on ABS after acetone vapor bath?]]></title>
			<link>https://www.soliforum.com/post/122736/#p122736</link>
			<description><![CDATA[<p>Now, now. Ian can&#039;t help it if he&#039;s insecure.</p>]]></description>
			<author><![CDATA[null@example.com (Heartlander)]]></author>
			<pubDate>Thu, 12 May 2016 12:33:06 +0000</pubDate>
			<guid>https://www.soliforum.com/post/122736/#p122736</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to get a matte finish on ABS after acetone vapor bath?]]></title>
			<link>https://www.soliforum.com/post/122712/#p122712</link>
			<description><![CDATA[<p>His link works, you just need to remove the s from the HTTP since it is not secure.</p><p><a href="http://solidoodletips.wordpress.com/2012/10/17/tumbler-finishing/">http://solidoodletips.wordpress.com/201 … finishing/</a></p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Thu, 12 May 2016 00:40:56 +0000</pubDate>
			<guid>https://www.soliforum.com/post/122712/#p122712</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to get a matte finish on ABS after acetone vapor bath?]]></title>
			<link>https://www.soliforum.com/post/122711/#p122711</link>
			<description><![CDATA[<p>I have been thinking of doing vapor blasting.<br />a friend of mine has the setup and uses extremely fine grit in his. ( like flower)<br />here is a good article on the process.</p><p><a href="http://www.vaporblastingequipment.com/wet-blasting/what-wetblasting-guide-vapor-blasting-process">http://www.vaporblastingequipment.com/w … ng-process</a></p><p>Note: Ians link is broken</p>]]></description>
			<author><![CDATA[null@example.com (dubbsd)]]></author>
			<pubDate>Thu, 12 May 2016 00:33:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/122711/#p122711</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to get a matte finish on ABS after acetone vapor bath?]]></title>
			<link>https://www.soliforum.com/post/122683/#p122683</link>
			<description><![CDATA[<p>Ceramic</p><p><a href="http://%20https://solidoodletips.wordpress.com/2012/10/17/tumbler-finishing/"> https://solidoodletips.wordpress.com/2 … finishing/</a></p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Wed, 11 May 2016 17:36:30 +0000</pubDate>
			<guid>https://www.soliforum.com/post/122683/#p122683</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to get a matte finish on ABS after acetone vapor bath?]]></title>
			<link>https://www.soliforum.com/post/122679/#p122679</link>
			<description><![CDATA[<p>That&#039;s a good idea. What media would you put in it?</p>]]></description>
			<author><![CDATA[null@example.com (Heartlander)]]></author>
			<pubDate>Wed, 11 May 2016 17:22:08 +0000</pubDate>
			<guid>https://www.soliforum.com/post/122679/#p122679</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to get a matte finish on ABS after acetone vapor bath?]]></title>
			<link>https://www.soliforum.com/post/122678/#p122678</link>
			<description><![CDATA[<p>Tumbling will take off the gloss and give it a nice soft finish.&nbsp; It&#039;s not very effective for smoothing,&nbsp; but it&#039;s a good followup to acetone.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Wed, 11 May 2016 17:17:01 +0000</pubDate>
			<guid>https://www.soliforum.com/post/122678/#p122678</guid>
		</item>
		<item>
			<title><![CDATA[How to get a matte finish on ABS after acetone vapor bath?]]></title>
			<link>https://www.soliforum.com/post/122660/#p122660</link>
			<description><![CDATA[<p>Gloss is fine but sometimes a flat finish would look better. Any ideas how to do that, short of spraying Testors Dull Coat?</p>]]></description>
			<author><![CDATA[null@example.com (Heartlander)]]></author>
			<pubDate>Wed, 11 May 2016 14:16:07 +0000</pubDate>
			<guid>https://www.soliforum.com/post/122660/#p122660</guid>
		</item>
	</channel>
</rss>