<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Acrylic frame assembly errata]]></title>
		<link>https://www.soliforum.com/topic/14408/acrylic-frame-assembly-errata/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/14408/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Acrylic frame assembly errata.]]></description>
		<lastBuildDate>Tue, 19 Apr 2016 01:24:11 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Acrylic frame assembly errata]]></title>
			<link>https://www.soliforum.com/post/121368/#p121368</link>
			<description><![CDATA[<p>I do the cutting for Uriah, its done on a 60w LC6040 laser cutter. I cut at about 8mm/sec, and it takes around 40 minutes to do an entire enclosure. Let me know if you have more questions!</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Tue, 19 Apr 2016 01:24:11 +0000</pubDate>
			<guid>https://www.soliforum.com/post/121368/#p121368</guid>
		</item>
		<item>
			<title><![CDATA[Re: Acrylic frame assembly errata]]></title>
			<link>https://www.soliforum.com/post/121365/#p121365</link>
			<description><![CDATA[<p>Not really errata, but wasn&#039;t sure where else to post it:</p><p>I really like the laser-cut acrylic enclosure.&nbsp; I&#039;m quite impressed with the forethought that went into designing this.&nbsp; I&#039;d be interested to learn about the laser cutter used, how long it takes to make the pieces, and any &#039;lessons learned&#039; for someone who&#039;s thinking of getting a laser cutter/engraver to complement my 3D printing capabilities.</p><p>Thanks.</p><p>-Kevin</p>]]></description>
			<author><![CDATA[null@example.com (knowack)]]></author>
			<pubDate>Tue, 19 Apr 2016 01:16:59 +0000</pubDate>
			<guid>https://www.soliforum.com/post/121365/#p121365</guid>
		</item>
		<item>
			<title><![CDATA[Re: Acrylic frame assembly errata]]></title>
			<link>https://www.soliforum.com/post/120134/#p120134</link>
			<description><![CDATA[<p>Ok thank you - I&#039;ll keep going then on that basis, both the assembly instructions and the video have been very useful, and if I notice anything else as I proceed I&#039;ll follow-up further.&nbsp; These have only been a couple of minor things, but even so I paused due to having doubts.&nbsp; Cheers.</p>]]></description>
			<author><![CDATA[null@example.com (topdog)]]></author>
			<pubDate>Tue, 29 Mar 2016 04:03:57 +0000</pubDate>
			<guid>https://www.soliforum.com/post/120134/#p120134</guid>
		</item>
		<item>
			<title><![CDATA[Re: Acrylic frame assembly errata]]></title>
			<link>https://www.soliforum.com/post/120104/#p120104</link>
			<description><![CDATA[<p>Recently, there were some minor changes made to the acrylic design based on customer feedback.&nbsp; It is easier to assemble (such as a single size acrylic spacer instead of two) and the design is stronger so that it is better with rough international shipping.&nbsp; The older version used 3 of the Pi&#039;s mounting holes while the newer version uses all 4.&nbsp; The video was of the newer design but the differences are minimal.</p><p>- Uriah</p>]]></description>
			<author><![CDATA[null@example.com (hairu526)]]></author>
			<pubDate>Mon, 28 Mar 2016 23:05:38 +0000</pubDate>
			<guid>https://www.soliforum.com/post/120104/#p120104</guid>
		</item>
		<item>
			<title><![CDATA[Acrylic frame assembly errata]]></title>
			<link>https://www.soliforum.com/post/120007/#p120007</link>
			<description><![CDATA[<p>With time I could probably figure these out with some process of elimination and undo/redo work, however I&#039;m not sure, maybe I am just reading it wrong.&nbsp; Could it be possible to see if these are errors and what the corrections should be?</p><p>1. Item FT isn&#039;t showing on the parts list.<br />2. Step 8 says to take 4 screws and put them into 3 holes and then put the pi over the &#039;three&#039; screws.&nbsp; Note the video makes it look like all 4 are used the same.<br />3. Step 8 says to use the FT spacers (4 of them) but the bag H had 6 thin plastic circular washers that I am not sure are spacers (what are they for, I would guess to help avoid shorts, but where if there are 6).<br />4. Item FU on parts list says quantity is x1 only.<br />5. If there are differences between FT and FU spacers and they are in the same bag I am unsure what the differences are from looking over them quickly.<br />6. Video makes it seem, though it wasn&#039;t easy to make it out for sure, that the FU type spacers are between both the pi and frame, and between the electronics board and frame, is that correct?</p><p>Thanks.</p>]]></description>
			<author><![CDATA[null@example.com (topdog)]]></author>
			<pubDate>Sun, 27 Mar 2016 05:40:25 +0000</pubDate>
			<guid>https://www.soliforum.com/post/120007/#p120007</guid>