<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Cleaned Extruder head and LCD screen broke?]]></title>
		<link>https://www.soliforum.com/topic/13808/cleaned-extruder-head-and-lcd-screen-broke/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/13808/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Cleaned Extruder head and LCD screen broke?.]]></description>
		<lastBuildDate>Tue, 07 Jun 2016 18:18:36 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Cleaned Extruder head and LCD screen broke?]]></title>
			<link>https://www.soliforum.com/post/123852/#p123852</link>
			<description><![CDATA[<p>You both probably shorted the 12 volts at the heater to ground. Read the sticky at the top of the XYZ section. There is a link near the end that explains what to do to fix the problem.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Tue, 07 Jun 2016 18:18:36 +0000</pubDate>
			<guid>https://www.soliforum.com/post/123852/#p123852</guid>
		</item>
		<item>
			<title><![CDATA[Re: Cleaned Extruder head and LCD screen broke?]]></title>
			<link>https://www.soliforum.com/post/123838/#p123838</link>
			<description><![CDATA[<p>did you figure out ? <br />I might have similar issue . <br />except I think I shorted board on top of the extruder</p>]]></description>
			<author><![CDATA[null@example.com (ap742)]]></author>
			<pubDate>Tue, 07 Jun 2016 14:24:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/123838/#p123838</guid>
		</item>
		<item>
			<title><![CDATA[Cleaned Extruder head and LCD screen broke?]]></title>
			<link>https://www.soliforum.com/post/117119/#p117119</link>
			<description><![CDATA[<p>Had a problem with a clogged extruder.</p><p>So I removed it and soaked it in some acetone.</p><p>Fitted it back together and the little screen at the front has stopped working.</p><p>Is there a wire I could have accidently pulled?</p>]]></description>
			<author><![CDATA[null@example.com (crazyewok)]]></author>
			<pubDate>Sun, 21 Feb 2016 17:29:46 +0000</pubDate>