<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Davinci Duo HIPS getting stuck in nozzle]]></title>
		<link>https://www.soliforum.com/topic/13446/davinci-duo-hips-getting-stuck-in-nozzle/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/13446/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Davinci Duo HIPS getting stuck in nozzle.]]></description>
		<lastBuildDate>Sat, 23 Jan 2016 06:51:04 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Davinci Duo HIPS getting stuck in nozzle]]></title>
			<link>https://www.soliforum.com/post/114846/#p114846</link>
			<description><![CDATA[<p>So far seems the head is the issue. Replaced and seems to work well.</p><p><a href="http://www.soliforum.com/post/114842/#p114842">http://www.soliforum.com/post/114842/#p114842</a></p>]]></description>
			<author><![CDATA[null@example.com (kszwab)]]></author>
			<pubDate>Sat, 23 Jan 2016 06:51:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/114846/#p114846</guid>
		</item>
		<item>
			<title><![CDATA[Re: Davinci Duo HIPS getting stuck in nozzle]]></title>
			<link>https://www.soliforum.com/post/114845/#p114845</link>
			<description><![CDATA[<p>I have been printing with HIPS on my version 1.0. Since I&#039;m making the filament it&#039;s only 1.65mm, so has given me no issue&#039;s.</p><p>Since you mentioned some of the filament your using is &quot;home made&quot; you might want to see if undersizing would fix your issue. I&#039;m currently printing with Craftware most of the time, but any non stock slicer would let you set the filament size as you wish, so printing with a slightly smaller filament is not a problem.</p>]]></description>
			<author><![CDATA[null@example.com (Weekend Avenger)]]></author>
			<pubDate>Sat, 23 Jan 2016 06:49:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/114845/#p114845</guid>
		</item>
		<item>
			<title><![CDATA[Re: Davinci Duo HIPS getting stuck in nozzle]]></title>
			<link>https://www.soliforum.com/post/114814/#p114814</link>
			<description><![CDATA[<p>I believe something is screwed up in the left head of the Duo. No matter how much I clean it (I completely dissasembled it, including the heater block and heat pipe) it gets blocked after a while. I will replace it temporarily with a new spare I have to test if the same happens with various filaments (ABS, HIPS, Cicoloy home made crap) with temps between 220-240C.</p><p>The filament swells in the pipe (as if the temp was too high) and then I have to dissasemble it, take the pipe apart, drill the filament out (will not slide out), clean the inside of the heater block and drill the nozzle with a .4 mm drill. Very weird. I checked if there may be scratches on the inside of the heat pipe or debris, but all looks fine. I am thinking to hook up a 12V source to the old heater block to be able to clean it better when it would be at about 230C, maybe there is cooked plastic inside that I cannot see.</p><p>But what I really want is a more modular, teflon insulated head as the MK8, eventually replacing both heads.</p>]]></description>
			<author><![CDATA[null@example.com (kszwab)]]></author>
			<pubDate>Fri, 22 Jan 2016 21:52:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/114814/#p114814</guid>
		</item>
		<item>
			<title><![CDATA[Re: Davinci Duo HIPS getting stuck in nozzle]]></title>
			<link>https://www.soliforum.com/post/114446/#p114446</link>
			<description><![CDATA[<p>I lowered the temperature on both extruders to 220C, seems to be doing better.</p>]]></description>
			<author><![CDATA[null@example.com (kszwab)]]></author>
			<pubDate>Mon, 18 Jan 2016 23:52:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/114446/#p114446</guid>
		</item>
		<item>
			<title><![CDATA[Davinci Duo HIPS getting stuck in nozzle]]></title>
			<link>https://www.soliforum.com/post/114442/#p114442</link>
			<description><![CDATA[<p>I have been printing with HIPS for a few days and now I am getting problems. I am using the left extruder with HIPS at 230-240C and after a while the nozzle gets plugged, HARD. I have had three times now to completely dissasemble the head and drill out the stuck filament. I measured the stuck part to swell to about 2 mm from 1.75mm and it does not slide anymore.</p><p>Is this because of the shitty XYZ head that does not have a teflon sleeve ? I have a few extra radiators, but seems the heat creep is the culprit. If I print ABS only, no issue.</p><p>Should I lower the temp to 220C and try again ?</p><p>Did anyone print with HIPS with the original Davinci Duo head ?</p><p>Thanks.</p>]]></description>
			<author><![CDATA[null@example.com (kszwab)]]></author>
			<pubDate>Mon, 18 Jan 2016 23:25:12 +0000</pubDate>
			<guid>https://www.soliforum.com/post/114442/#p114442</guid>