<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Banging noises and warping]]></title>
		<link>https://www.soliforum.com/topic/13230/banging-noises-and-warping/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/13230/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Banging noises and warping.]]></description>
		<lastBuildDate>Thu, 31 Dec 2015 03:27:34 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Banging noises and warping]]></title>
			<link>https://www.soliforum.com/post/112956/#p112956</link>
			<description><![CDATA[<p>I get the banging noises in the front right of the build plate too, mostly when doing the first couple of lines. Sometimes I can get it to be a little quieter if I gently help push the filament through. I don&#039;t know if the knocking or the assisting the filament is hurting anything.</p>]]></description>
			<author><![CDATA[null@example.com (artanangus)]]></author>
			<pubDate>Thu, 31 Dec 2015 03:27:34 +0000</pubDate>
			<guid>https://www.soliforum.com/post/112956/#p112956</guid>
		</item>
		<item>
			<title><![CDATA[Re: Banging noises and warping]]></title>
			<link>https://www.soliforum.com/post/112949/#p112949</link>
			<description><![CDATA[<p>It happens to me too. Seems to do it more so when printing around the front right corner of the build plate. In the beginning of the print since it prints the purge lines in that corner I always get the banging when the print starts.</p>]]></description>
			<author><![CDATA[null@example.com (reznor9)]]></author>
			<pubDate>Thu, 31 Dec 2015 01:30:32 +0000</pubDate>
			<guid>https://www.soliforum.com/post/112949/#p112949</guid>
		</item>
		<item>
			<title><![CDATA[Re: Banging noises and warping]]></title>
			<link>https://www.soliforum.com/post/112943/#p112943</link>
			<description><![CDATA[<div class="quotebox"><cite>jwalker55 wrote:</cite><blockquote><p>I had what I would describe as &quot;banging&quot; noises only on the first layer and i&#039;m guessing it was the extruder motor slipping.&nbsp; I increased the z-offset and it went away.</p></blockquote></div><p>Ok how do I do that?</p>]]></description>
			<author><![CDATA[null@example.com (crazyewok)]]></author>
			<pubDate>Wed, 30 Dec 2015 23:34:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/112943/#p112943</guid>
		</item>
		<item>
			<title><![CDATA[Re: Banging noises and warping]]></title>
			<link>https://www.soliforum.com/post/112935/#p112935</link>
			<description><![CDATA[<p>I had what I would describe as &quot;banging&quot; noises only on the first layer and i&#039;m guessing it was the extruder motor slipping.&nbsp; I increased the z-offset and it went away.</p>]]></description>
			<author><![CDATA[null@example.com (jwalker55)]]></author>
			<pubDate>Wed, 30 Dec 2015 21:52:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/112935/#p112935</guid>
		</item>
		<item>
			<title><![CDATA[Banging noises and warping]]></title>
			<link>https://www.soliforum.com/post/112921/#p112921</link>
			<description><![CDATA[<p>At the start of each print I get banging noises.&nbsp; Only at the start though as after 5 secounds its stops.</p><p>I am also getting warping on prints.</p><p>I have done the calibration and cleaned the extruder ect</p>]]></description>
			<author><![CDATA[null@example.com (crazyewok)]]></author>
			<pubDate>Wed, 30 Dec 2015 17:21:35 +0000</pubDate>
			<guid>https://www.soliforum.com/post/112921/#p112921</guid>
		</item>