		<title><![CDATA[SoliForum - 3D Printing Community — ABS PC VS ABS FR ?]]></title>
		<link>https://www.soliforum.com/topic/13065/abs-pc-vs-abs-fr/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/13065/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in ABS PC VS ABS FR ?.]]></description>
		<lastBuildDate>Fri, 11 Dec 2015 07:35:53 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: ABS PC VS ABS FR ?]]></title>
			<link>https://www.soliforum.com/post/111375/#p111375</link>
			<description><![CDATA[<p>hi<br />thx tim <br />can we mix pc &amp; fr pellets?</p>]]></description>
			<author><![CDATA[null@example.com (fredaxe)]]></author>
			<pubDate>Fri, 11 Dec 2015 07:35:53 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111375/#p111375</guid>
		</item>
		<item>
			<title><![CDATA[Re: ABS PC VS ABS FR ?]]></title>
			<link>https://www.soliforum.com/post/111318/#p111318</link>
			<description><![CDATA[<p>FR is flame resistant, PC means it is a blend of ABS and Polycarbonate.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Thu, 10 Dec 2015 16:40:14 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111318/#p111318</guid>
		</item>
		<item>
			<title><![CDATA[ABS PC VS ABS FR ?]]></title>
			<link>https://www.soliforum.com/post/111316/#p111316</link>
			<description><![CDATA[<p>hi all<br />someone tell me the difference between&nbsp; ABS FR &amp; ABS PC, please?</p><p>thx <br />fas83 as fredaxe</p>]]></description>
			<author><![CDATA[null@example.com (fredaxe)]]></author>
			<pubDate>Thu, 10 Dec 2015 16:07:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/111316/#p111316</guid>
		</item>