<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — E3DV6 25 or 40 watt heater cart?]]></title>
		<link>https://www.soliforum.com/topic/12715/e3dv6-25-or-40-watt-heater-cart/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/12715/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in E3DV6 25 or 40 watt heater cart?.]]></description>
		<lastBuildDate>Tue, 03 Nov 2015 05:24:02 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: E3DV6 25 or 40 watt heater cart?]]></title>
			<link>https://www.soliforum.com/post/108806/#p108806</link>
			<description><![CDATA[<p>Don&#039;t the installation instructions say to heat up to 285°C, and then tighten the nozzle?&nbsp; Since the 25W element gets you to 285°C, I think you&#039;re okay.&nbsp; If you haven&#039;t yet &#039;pre-heated&#039; the E3Dv6 IAW the instructions, save yourself some heartache, and do it before you start running filament through it.</p>]]></description>
			<author><![CDATA[null@example.com (knowack)]]></author>
			<pubDate>Tue, 03 Nov 2015 05:24:02 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108806/#p108806</guid>
		</item>
		<item>
			<title><![CDATA[Re: E3DV6 25 or 40 watt heater cart?]]></title>
			<link>https://www.soliforum.com/post/108802/#p108802</link>
			<description><![CDATA[<p>I have printed with ABS PLA TPU AND TPEG. I have taken the hot end to 300 c with that heater cart.&nbsp; had it that hot when I was doing the final tightening of the nozzle. as you want it hot when you do that</p>]]></description>
			<author><![CDATA[null@example.com (mark.burton)]]></author>
			<pubDate>Tue, 03 Nov 2015 05:09:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108802/#p108802</guid>
		</item>
		<item>
			<title><![CDATA[Re: E3DV6 25 or 40 watt heater cart?]]></title>
			<link>https://www.soliforum.com/post/108796/#p108796</link>
			<description><![CDATA[<div class="quotebox"><cite>elmoret wrote:</cite><blockquote><p>25 watt heater cartridge is good to over 300C.</p></blockquote></div><br /><p>Thanks, then I think I will be good.&nbsp; <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></description>
			<author><![CDATA[null@example.com (mpoffo)]]></author>
			<pubDate>Tue, 03 Nov 2015 04:11:41 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108796/#p108796</guid>
		</item>
		<item>
			<title><![CDATA[Re: E3DV6 25 or 40 watt heater cart?]]></title>
			<link>https://www.soliforum.com/post/108781/#p108781</link>
			<description><![CDATA[<p>25 watt heater cartridge is good to over 300C.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Tue, 03 Nov 2015 02:52:25 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108781/#p108781</guid>
		</item>
		<item>
			<title><![CDATA[Re: E3DV6 25 or 40 watt heater cart?]]></title>
			<link>https://www.soliforum.com/post/108777/#p108777</link>
			<description><![CDATA[<p>Thanks I appreciate the replies.&nbsp; Mark have you had any issues getting the higher temps?&nbsp; What types of filament have you used (ie ABS, PLA, Ninja Flex, etc) ?</p>]]></description>
			<author><![CDATA[null@example.com (mpoffo)]]></author>
			<pubDate>Tue, 03 Nov 2015 02:08:01 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108777/#p108777</guid>
		</item>
		<item>
			<title><![CDATA[Re: E3DV6 25 or 40 watt heater cart?]]></title>
			<link>https://www.soliforum.com/post/108751/#p108751</link>
			<description><![CDATA[<p>I am using the heater cart that came with my e3d its the 12 volt 25 watt and I haven&#039;t had any problems.</p>]]></description>
			<author><![CDATA[null@example.com (mark.burton)]]></author>
			<pubDate>Mon, 02 Nov 2015 22:42:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108751/#p108751</guid>
		</item>
		<item>
			<title><![CDATA[Re: E3DV6 25 or 40 watt heater cart?]]></title>
			<link>https://www.soliforum.com/post/108748/#p108748</link>
			<description><![CDATA[<p>Why not reuse the stock heater cartridge?</p>]]></description>
			<author><![CDATA[null@example.com (evanalmighty)]]></author>
			<pubDate>Mon, 02 Nov 2015 22:13:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108748/#p108748</guid>
		</item>
		<item>
			<title><![CDATA[E3DV6 25 or 40 watt heater cart?]]></title>
			<link>https://www.soliforum.com/post/108747/#p108747</link>
			<description><![CDATA[<p>I am wondering if the 25 watt heater cart (blue wires) that came with my E3D V6 is sufficient?&nbsp; I can get a 12 V 40 watt one (red wires) if it would be better.&nbsp; If I do would the default power supply be sufficient?</p><p>I have a upgraded glass bed, will be repurposing the fan on the DaVinci and will have the additional fan attached to the E3D V6.&nbsp; Nothing else added.</p><p>If the 25W will work well then I will stick with it.&nbsp; I simply have not had time to complete this upgrade yet and want to avoid having to take things apart to change the heater cart.</p><p>Thanks</p><p>Mark</p>]]></description>