<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Does natural ABS print out as "white"?]]></title>
		<link>https://www.soliforum.com/topic/12691/does-natural-abs-print-out-as-white/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/12691/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Does natural ABS print out as "white"?.]]></description>
		<lastBuildDate>Fri, 30 Oct 2015 06:29:54 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Does natural ABS print out as "white"?]]></title>
			<link>https://www.soliforum.com/post/108559/#p108559</link>
			<description><![CDATA[<div class="quotebox"><cite>elmoret wrote:</cite><blockquote><p>Natural ABS is off-white, it will come out the same color as it goes in.</p><p>Clear ABS isn&#039;t really ABS at all. Here&#039;s a nice discussion on it:</p><p><a href="http://forums.reprap.org/read.php?1,150410,216683">http://forums.reprap.org/read.php?1,150410,216683</a></p></blockquote></div><p>Correct, if you want true white, you need to add white colourant.&nbsp; For most purposes natural might be sufficient though.&nbsp; As far as I know most of the people who buy colourant from me use the might to lighten other colours and just use natural for pseudo white printing.&nbsp; But natural is more like a dirty off-white as you will have noted from the pellets.</p>]]></description>
			<author><![CDATA[null@example.com (CraigRK)]]></author>
			<pubDate>Fri, 30 Oct 2015 06:29:54 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108559/#p108559</guid>
		</item>
		<item>
			<title><![CDATA[Re: Does natural ABS print out as "white"?]]></title>
			<link>https://www.soliforum.com/post/108553/#p108553</link>
			<description><![CDATA[<p>Natural ABS is off-white, it will come out the same color as it goes in.</p><p>Clear ABS isn&#039;t really ABS at all. Here&#039;s a nice discussion on it:</p><p><a href="http://forums.reprap.org/read.php?1,150410,216683">http://forums.reprap.org/read.php?1,150410,216683</a></p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Fri, 30 Oct 2015 04:18:36 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108553/#p108553</guid>
		</item>
		<item>
			<title><![CDATA[Does natural ABS print out as "white"?]]></title>
			<link>https://www.soliforum.com/post/108552/#p108552</link>
			<description><![CDATA[<p>Just wondering. I see natural ABS often referred to as &quot;Clear ABS&quot;, but it looks pretty white to me. Does it print out as something white or something not-quite-white? I&#039;m not sure if I need to add this &quot;shimmering white&quot; ABS colorant or not to get regular white ABS filament; I&#039;d rather not if I don&#039;t have to.</p>]]></description>
			<author><![CDATA[null@example.com (swbluto4gems)]]></author>
			<pubDate>Fri, 30 Oct 2015 04:10:33 +0000</pubDate>
			<guid>https://www.soliforum.com/post/108552/#p108552</guid>
		</item>
	</channel>
</rss>