<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Couple questions about my solidoodle 4...]]></title>
		<link>https://www.soliforum.com/topic/12474/couple-questions-about-my-solidoodle-4/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/12474/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Couple questions about my solidoodle 4....]]></description>
		<lastBuildDate>Tue, 06 Oct 2015 15:05:07 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Couple questions about my solidoodle 4...]]></title>
			<link>https://www.soliforum.com/post/107080/#p107080</link>
			<description><![CDATA[<div class="quotebox"><cite>Tin Falcon wrote:</cite><blockquote><p>I too have had an SD 4 for about 1 year. <br />Setting the steps per mm is easy via the RH host software. You do not need to reflash firmware to adjust steps. <br />Tin</p></blockquote></div><p>not looking to reflash firmware to adjust steps, i reflashed already because the bed dimensions were wrong &amp; i wanted to enable thermal runaway protection -- but thermal runaway protection has some issues in this version (<a href="https://github.com/ozadr1an/Solidoodle-Marlin_v1/tree/Solidoodle_Marlin_v1_beta">https://github.com/ozadr1an/Solidoodle- … in_v1_beta</a>), and looking at release notes those issues have been resolved in later marlin releases.</p>]]></description>
			<author><![CDATA[null@example.com (GMBridge)]]></author>
			<pubDate>Tue, 06 Oct 2015 15:05:07 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107080/#p107080</guid>
		</item>
		<item>
			<title><![CDATA[Re: Couple questions about my solidoodle 4...]]></title>
			<link>https://www.soliforum.com/post/107073/#p107073</link>
			<description><![CDATA[<p>I too have had an SD 4 for about 1 year. <br />Setting the steps per mm is easy via the RH host software. You do not need to reflash firmware to adjust steps. <br />Tin</p>]]></description>
			<author><![CDATA[null@example.com (Tin Falcon)]]></author>
			<pubDate>Tue, 06 Oct 2015 10:55:10 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107073/#p107073</guid>
		</item>
		<item>
			<title><![CDATA[Re: Couple questions about my solidoodle 4...]]></title>
			<link>https://www.soliforum.com/post/107020/#p107020</link>
			<description><![CDATA[<p>1. Yes! definitely need to adjust the steps per mm for the extruder. Solidoodle sets it FAR to high. should be more like 102-105 vs the 138 they have it set at.<br />Measure and mark 100mms on the filament feeding into the extruder top (you may want to make a second mark at 150mms). in RH free extrude 100mms - measure how much it fed past the 100mm mark (or how much remains to the 150mm mark) <br />use this formula to calculate the corrected steps/mm:<br />&nbsp; &nbsp; &nbsp;(expected length* x current steps per mm) / actual length = new steps per mm.<br />&nbsp; &nbsp; &nbsp; &nbsp; &nbsp; *expected length is the 100mm you asked for</p><p>2. If you are using the stock hotend, then yes, the fan on the side is necessary to keep the cool side of the hotend cool enough to prevent heat-creep and internal meltdown of the PEEK liner. If you upgrade the hotend to an all metal like the E3D v6, then it could be removed.</p><p>3. I have no experience flashing the Printrboard, so cant really comment on that one, but i see no reason why you couldn&#039;t. Others here have more experience with this.</p>]]></description>
			<author><![CDATA[null@example.com (heartless)]]></author>
			<pubDate>Mon, 05 Oct 2015 14:56:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107020/#p107020</guid>
		</item>
		<item>
			<title><![CDATA[Couple questions about my solidoodle 4...]]></title>
			<link>https://www.soliforum.com/post/107015/#p107015</link>
			<description><![CDATA[<p>had my solidoodle4 for about a year now, pushed a couple kilo&#039;s of filament through it at this point.</p><p>1. so, my extrusion % is set to like 66%, should i just redo my extruder&#039;s steps per mm to get that closer to 100%, and just use extrusion % for fine adjustments?</p><p>2. is the fan on the side of the extruder head necessary?</p><p>3. can i compile mainline marlin firmware for the printrboard, or do i need to use the year+ old &quot;special&quot; marlin firmware branch linked here? (it looks like there would just be some lines to be copied over from the config.h file)</p>]]></description>