<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — printer head tool snapped off in nozzle]]></title>
		<link>https://www.soliforum.com/topic/11542/printer-head-tool-snapped-off-in-nozzle/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/11542/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in printer head tool snapped off in nozzle.]]></description>
		<lastBuildDate>Sat, 20 Jun 2015 08:08:34 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: printer head tool snapped off in nozzle]]></title>
			<link>https://www.soliforum.com/post/99494/#p99494</link>
			<description><![CDATA[<p>Thanks-sorry didn&#039;t mean to post multiple times. Deleted extras.<br />My concern is that the item that is stuck now is metal and if I put in filament and heat it it may have the effect of gluing in the littel metal piece. I guess it couldn&#039;t hurt at this point. If that fails does anyone know if Best Buy can repair these sort of units or where I can go to get it repaired.?</p><p>Even though it is metal stuck in there do you think heating and extruding might get it out?</p><p> thanks<br />&nbsp; </p><div class="quotebox"><cite>carl_m1968 wrote:</cite><blockquote><div class="quotebox"><cite>Danthefisherman wrote:</cite><blockquote><p>I have a xyz 3d printer and the nozzle cleaning tool .4mm snapped off in the printer nozzle/extruder. i haven&#039;t been able to get it out. Any suggestions? thanks</p></blockquote></div><p>[quote You may have cleared it enough that you could try to heat and extrude it.</p></blockquote></div>]]></description>
			<author><![CDATA[null@example.com (Danthefisherman)]]></author>
			<pubDate>Sat, 20 Jun 2015 08:08:34 +0000</pubDate>
			<guid>https://www.soliforum.com/post/99494/#p99494</guid>
		</item>
		<item>
			<title><![CDATA[Re: printer head tool snapped off in nozzle]]></title>
			<link>https://www.soliforum.com/post/99493/#p99493</link>
			<description><![CDATA[<div class="quotebox"><cite>Danthefisherman wrote:</cite><blockquote><p>I have a xyz 3d printer and the nozzle cleaning tool .4mm snapped off in the printer nozzle/extruder. i haven&#039;t been able to get it out. Any suggestions? thanks</p></blockquote></div><p>You may have cleared it enough that you could try to heat and extrude it.</p><p>By the way, you only need to post once. No one works here but we as users will try to answer you as soon as life permits.</p><p>So you might want to go back and delete the unanswered threads.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Sat, 20 Jun 2015 06:07:33 +0000</pubDate>
			<guid>https://www.soliforum.com/post/99493/#p99493</guid>
		</item>
		<item>
			<title><![CDATA[printer head tool snapped off in nozzle]]></title>
			<link>https://www.soliforum.com/post/99491/#p99491</link>
			<description><![CDATA[<p>I have a xyz 3d printer and the nozzle cleaning tool .4mm snapped off in the printer nozzle/extruder. i haven&#039;t been able to get it out. Any suggestions? thanks</p>]]></description>
			<author><![CDATA[null@example.com (Danthefisherman)]]></author>
			<pubDate>Sat, 20 Jun 2015 05:34:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/99491/#p99491</guid>