<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — PTFE for extruder barrel]]></title>
		<link>https://www.soliforum.com/topic/11271/ptfe-for-extruder-barrel/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/11271/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in PTFE for extruder barrel.]]></description>
		<lastBuildDate>Mon, 25 May 2015 12:49:57 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: PTFE for extruder barrel]]></title>
			<link>https://www.soliforum.com/post/96948/#p96948</link>
			<description><![CDATA[<p>Try here...</p><p><a href="http://www.filastruder.com/collections/e3d-spare-parts-and-accessories">http://www.filastruder.com/collections/ … ccessories</a></p><p>about halfway down the page in the center.</p>]]></description>
			<author><![CDATA[null@example.com (Ski52)]]></author>
			<pubDate>Mon, 25 May 2015 12:49:57 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96948/#p96948</guid>
		</item>
		<item>
			<title><![CDATA[PTFE for extruder barrel]]></title>
			<link>https://www.soliforum.com/post/96897/#p96897</link>
			<description><![CDATA[<p>Hello all,</p><p>From printing PET+ my PTFE tube in the extruder barrel wore out and i bought a new tube.<br />The thing is that now after putting the new tube printing the PET+ sometimes it extrudes with like pieces of the tube like its peeling the inside of it. I put some baby oil on the fillament and it has improved. The original seemed alot more robust, any suggestion on where to get some PTFE tube?</p><p>Thanks</p>]]></description>
			<author><![CDATA[null@example.com (eduardogarcia3049)]]></author>
			<pubDate>Sun, 24 May 2015 17:37:07 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96897/#p96897</guid>
		</item>
	</channel>
</rss>