<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Kapton Tape]]></title>
		<link>https://www.soliforum.com/topic/11175/kapton-tape/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/11175/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Kapton Tape.]]></description>
		<lastBuildDate>Mon, 18 May 2015 21:19:49 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Kapton Tape]]></title>
			<link>https://www.soliforum.com/post/96191/#p96191</link>
			<description><![CDATA[<p>Makerbot sends them out with the Replicator 2X.<br />Dog got a hold of mine (Chew Toy)</p>]]></description>
			<author><![CDATA[null@example.com (dubbsd)]]></author>
			<pubDate>Mon, 18 May 2015 21:19:49 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96191/#p96191</guid>
		</item>
		<item>
			<title><![CDATA[Re: Kapton Tape]]></title>
			<link>https://www.soliforum.com/post/96129/#p96129</link>
			<description><![CDATA[<p>Here is the preferred tool . Made for aplying vynl signs.<br /><a href="http://www.ebay.com/itm/like/261802407956?lpid=82&amp;chn=ps">http://www.ebay.com/itm/like/2618024079 … amp;chn=ps</a></p><p><span class="postimg"><img src="http://i.ebayimg.com/00/s/MTAxMFgxMDEw/z/8lkAAOSw6EhUO55C/$_35.JPG" alt="http://i.ebayimg.com/00/s/MTAxMFgxMDEw/z/8lkAAOSw6EhUO55C/$_35.JPG" /></span></p><p>tin</p>]]></description>
			<author><![CDATA[null@example.com (Tin Falcon)]]></author>
			<pubDate>Mon, 18 May 2015 10:56:52 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96129/#p96129</guid>
		</item>
		<item>
			<title><![CDATA[Re: Kapton Tape]]></title>
			<link>https://www.soliforum.com/post/96125/#p96125</link>
			<description><![CDATA[<p>I use bondo spatulas they are cheaper than breaking a credit card. Start at one&nbsp; end of the bed&nbsp; and lay the tape using the spatula as you go</p>]]></description>
			<author><![CDATA[null@example.com (dubbsd)]]></author>
			<pubDate>Mon, 18 May 2015 09:47:46 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96125/#p96125</guid>
		</item>
		<item>
			<title><![CDATA[Re: Kapton Tape]]></title>
			<link>https://www.soliforum.com/post/96124/#p96124</link>
			<description><![CDATA[<p>You could use the wet method to apply the tape.</p><p>I spray window cleaner on the glass, then apply the tape, and use credit card to move all bubbles to the sides and out. Let it dry (you could try heating the bed to evaporate all remaining liquid). This results in a perfectly applied Kapton tape.</p><p>You can also find some instructional videos on youtube.</p>]]></description>
			<author><![CDATA[null@example.com (domas)]]></author>
			<pubDate>Mon, 18 May 2015 09:29:31 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96124/#p96124</guid>
		</item>
		<item>
			<title><![CDATA[Re: Kapton Tape]]></title>
			<link>https://www.soliforum.com/post/96108/#p96108</link>
			<description><![CDATA[<div class="quotebox"><cite>helimwyatt wrote:</cite><blockquote><p>So what&#039;s the trick to apply Kapton tape without bubbles? I bought an eight inch wide roll for the press, but what a pain to apply!</p></blockquote></div><p>Use two inch wide and apply strips next to each other smoothing as you lay them. Just use it in the area that the print will be in. or use Elmers purple glue stick. It works far better than Kapton and is much easier to apply.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Mon, 18 May 2015 04:46:08 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96108/#p96108</guid>
		</item>
		<item>
			<title><![CDATA[Kapton Tape]]></title>
			<link>https://www.soliforum.com/post/96107/#p96107</link>
			<description><![CDATA[<p>So what&#039;s the trick to apply Kapton tape without bubbles? I bought an eight inch wide roll for the press, but what a pain to apply!</p>]]></description>