<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Filament - ZeroCart]]></title>
		<link>https://www.soliforum.com/topic/10625/filament-zerocart/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/10625/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Filament - ZeroCart.]]></description>
		<lastBuildDate>Wed, 01 Apr 2015 00:54:10 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Filament - ZeroCart]]></title>
			<link>https://www.soliforum.com/post/91605/#p91605</link>
			<description><![CDATA[<div class="quotebox"><cite>galaxy99 wrote:</cite><blockquote><p>Perhaps I wasn&#039;t clear - yes, there is close to 400m on a 1kg spool, that&#039;s the purpose for both 240m and 160m (=400). With these two, user can accurately track usage. But, most of us can do the math so, when I get to the end of 240m, knowing ~160m remains, I don&#039;t bother with changing the Zerocart/CoolTerm - I simply do a new Cartridge load and know (and write down) there is actually 160m on the spool, and not 240m.</p><p>I indicated the different choices for those who use iPhones and forgot 1+1 = 2.&nbsp; Actually, even that can be cleverly put, see the attached file...</p></blockquote></div><p> Oh yea I forgot I was the last and only android/pc user in the world. I apologize for expressing my ignorance. </p><p>I chose to reflash my Da vinci so I wont be challanged by math. I currently am dumping the stock board for an Azteeg X5 so I dont even have to deal Audrino. </p><p>But then again not having an iPhone I guess I habe to dumb all my stuff down to my Ievel:)</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Wed, 01 Apr 2015 00:54:10 +0000</pubDate>
			<guid>https://www.soliforum.com/post/91605/#p91605</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament - ZeroCart]]></title>
			<link>https://www.soliforum.com/post/91603/#p91603</link>
			<description><![CDATA[<p>Perhaps I wasn&#039;t clear - yes, there is close to 400m on a 1kg spool, that&#039;s the purpose for both 240m and 160m (=400). With these two, user can accurately track usage. But, most of us can do the math so, when I get to the end of 240m, knowing ~160m remains, I don&#039;t bother with changing the Zerocart/CoolTerm - I simply do a new Cartridge load and know (and write down) there is actually 160m on the spool, and not 240m.</p><p>I indicated the different choices for those who use iPhones and forgot 1+1 = 2.&nbsp; Actually, even that can be cleverly put, see the attached file...</p>]]></description>
			<author><![CDATA[null@example.com (galaxy99)]]></author>
			<pubDate>Wed, 01 Apr 2015 00:23:36 +0000</pubDate>
			<guid>https://www.soliforum.com/post/91603/#p91603</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament - ZeroCart]]></title>
			<link>https://www.soliforum.com/post/91601/#p91601</link>
			<description><![CDATA[<p>Your first option is cheating you out of 100 meters. In most 1kg spools there is about 340 meters on it. Remember XYZ tips you off by selling a 600g spool for the same price as the other guys 1kg. So you have to adjust.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Wed, 01 Apr 2015 00:06:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/91601/#p91601</guid>
		</item>
		<item>
			<title><![CDATA[Filament - ZeroCart]]></title>
			<link>https://www.soliforum.com/post/91600/#p91600</link>
			<description><![CDATA[<p>Thought I’d mention:</p><p>Using CoolTerm to make Zerocart settings.</p><ul><li><p>Without downgrading firmware, the printer only recognizes max Length (Zerocart setting) of 240m.</p></li><li><p>The printer will use the last file saved to the Zerocart when you Load a new spool.</p></li></ul><ul><li><p>Setup three files in CoolTerm (using 1kg spool of Shaxon Black for this example):</p></li><li><p>240m Black_Shax</p></li><li><p>160m Black_Shax_Remainder</p></li><li><p>100m Mixed Shax</p></li></ul><p><strong>Now, when you load a new spool, you have Two choices:</strong><br /> 1 - Load the filament and use the Last file set in Zerocart (assume it was the 240m).&nbsp; if your new spool or remainder of existing spool has less, than 240m, use your tracking log (you are logging it, right?) to determine how much remains.</p><p>Note, the amount used shown in the LCD is correct so you can subtract that from the amount you logged for the actual remaining amount.</p><p>Or,<br /> 2 - Load the filament and use the CoolTerm file “…Remainder” for the remaining amount.</p><p><strong>But,</strong> If you do choice#2, you’ll need to reload the CoolTerm file for the full amount next time you load a full spool.<br />Hence, just stick with Choice#1.&nbsp; If you don’t care about the color the pinter thinks is loaded (and why would you, it has nothing to do with the print) well, you simply won’t ever need to mess with CoolTerm again!</p><p><strong><span style="color: red">A bonus:</span></strong> if you have a few meters of filament and/or, if you have colors you want to mix in a print, you can:</p><p>Load the filament and use the CoolTerm file “…Mixed”.&nbsp; (use the Mixed file so there won’t be subtractions from the 240m or 160m files).&nbsp; You can print as much or as little of your shorter lengths but, the best part is, you can clean-cut the current filament and Chase it with a different color while printing without Unloading or Loading.&nbsp; Just be sure to Chase it without a gap between the different filaments until it starts feeding by itself - No Dual extruder needed for multi-colored parts!</p>]]></description>