			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/84008/#p84008" />
			<content type="html"><![CDATA[<p>Glad you finally figured it out.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-08T03:55:23Z</updated>
			<id>https://www.soliforum.com/post/84008/#p84008</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83984/#p83984" />
			<content type="html"><![CDATA[<p>FINALLY!!!</p><p>Well it looks like that new firmware version fixed it.&nbsp; Here is my first completely printed part!</p><p>Thank you all for your help!</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-08T01:09:16Z</updated>
			<id>https://www.soliforum.com/post/83984/#p83984</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83971/#p83971" />
			<content type="html"><![CDATA[<p>Okay, so that was a version that was jsut released then.&nbsp; No wonder I had the wrong one.&nbsp; Glad they fixed it.</p><p>It has been printing for 8 minutes now.&nbsp; The print has about 30 minutes left, but that is at least a few minutes longer than it has printed thus far.</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-07T23:39:45Z</updated>
			<id>https://www.soliforum.com/post/83971/#p83971</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83969/#p83969" />
			<content type="html"><![CDATA[<p>Another user had the same problem and this was the fix.<br /><a href="http://www.soliforum.com/topic/9691/help-printer-stops-extruding-about-an-hour-into-print/page/3/">http://www.soliforum.com/topic/9691/hel … nt/page/3/</a></p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-07T23:25:33Z</updated>
			<id>https://www.soliforum.com/post/83969/#p83969</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83968/#p83968" />
			<content type="html"><![CDATA[<p>I just downloaded the firmware that was in the instructions.&nbsp; I will give this a shot.</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-07T23:14:43Z</updated>
			<id>https://www.soliforum.com/post/83968/#p83968</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83966/#p83966" />
			<content type="html"><![CDATA[<p>I think you downloaded the M600 version and you want<br />This one.&nbsp; <br /><a href="https://github.com/ozadr1an/Solidoodle-Marlin_v1/blob/Solidoodle_Marlin_v1_beta/Marlin/Configuration.h">https://github.com/ozadr1an/Solidoodle- … guration.h</a><br />I think you are running into a problem with the filament alarm section that is in the M600 version.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-07T22:59:55Z</updated>
			<id>https://www.soliforum.com/post/83966/#p83966</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83963/#p83963" />
			<content type="html"><![CDATA[<p>Okay, working on that.&nbsp; I have to wait until my phone charges so that I can use the flash.</p><p>I did put an E3D on it and changed the firmware successfully - posted on page 2 I think - please feel free to look at it closely.</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-07T22:52:17Z</updated>
			<id>https://www.soliforum.com/post/83963/#p83963</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83959/#p83959" />
			<content type="html"><![CDATA[<p>Can you post a picture of the connectors?<br />Also (and forgive me if we&#039;ve covered this) have you done anything on the heater side of things?<br />What version of firmware are you using?&nbsp; E3d?</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-07T22:40:51Z</updated>
			<id>https://www.soliforum.com/post/83959/#p83959</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83958/#p83958" />
			<content type="html"><![CDATA[<p>Okay, fair enough, but I have replaced every wire within the thermistor line twice and tested them for continuity more times than I have hugged my children. </p><p>Any suggestions?</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-07T22:38:24Z</updated>
			<id>https://www.soliforum.com/post/83958/#p83958</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83957/#p83957" />
			<content type="html"><![CDATA[<p>Cold extrusion error is most likely a bad wire or loose connection.&nbsp; As the extruder wiggles around it is causing this error.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-07T22:36:50Z</updated>
			<id>https://www.soliforum.com/post/83957/#p83957</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83953/#p83953" />
			<content type="html"><![CDATA[<p>No luck, no luck at all.&nbsp; I will attach the screen shot but it is doing the EXACT same thing that it was doing before.&nbsp; Starts beautifully and then dies after a few minutes.</p><p>In two weeks I have not solved anything.</p><p>Temperature curve attached.</p><p>Anyone?</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-07T22:31:28Z</updated>
			<id>https://www.soliforum.com/post/83953/#p83953</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83951/#p83951" />
			<content type="html"><![CDATA[<p>Okay, it was the connector on the thermistor.&nbsp; Took it off and attached the wires sans connectors and it has started working.&nbsp; </p><p>first print in progress.&nbsp; Keep your fingers crossed.</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-07T22:08:20Z</updated>
			<id>https://www.soliforum.com/post/83951/#p83951</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83943/#p83943" />
			<content type="html"><![CDATA[<p>Finally got my screw in thermistor from printed solid in.&nbsp; &quot;Great&quot; you might say except that apparently something is wrong with it as I can not get a reading across the terminals at all.&nbsp; I double checked all of the wiring then finally pulled the thermistor and read it at the connector.&nbsp; No Ohm reading, no continuity, nothing.</p><p>You have got to be kidding me.</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-07T21:12:11Z</updated>
			<id>https://www.soliforum.com/post/83943/#p83943</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83652/#p83652" />
			<content type="html"><![CDATA[<p>Yup, I have been there many times myself over the last couple of months.&nbsp; There are times where I have to completely walk away from it for a week or so.</p><p>But I am so close to getting it right...</p>]]></content>
			<author>
				<name><![CDATA[brandon]]></name>
				<uri>https://www.soliforum.com/user/8559/</uri>
			</author>
			<updated>2015-02-06T17:21:39Z</updated>
			<id>https://www.soliforum.com/post/83652/#p83652</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temperature dropping out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83584/#p83584" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>brandon wrote:</cite><blockquote><p>I am sure that a lot of people here are more qualified than me to answer this, but maybe try following the steps I went through on the heater: checking voltage on the pins coming out from the board and checking the resistance of the heater itself.</p></blockquote></div><p>My heat wasn&#039;t dropping off like this until I tried to flash the updated firmware. Previously I had a steps/mm issue that I solved, then when I tried to update (which didn&#039;t take) my heat started dropping out like this. I&#039;m about ready to give this machine a viking funeral.</p>]]></content>
			<author>
				<name><![CDATA[fdm_process]]></name>
				<uri>https://www.soliforum.com/user/9405/</uri>
			</author>
			<updated>2015-02-06T03:39:55Z</updated>
			<id>https://www.soliforum.com/post/83584/#p83584</id>