<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Proper way to change filament in repetier host?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/9540/" />
	<updated>2015-01-31T13:44:48Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/9540/proper-way-to-change-filament-in-repetier-host/</id>
		<entry>
			<title type="html"><![CDATA[Re: Proper way to change filament in repetier host?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/82554/#p82554" />
			<content type="html"><![CDATA[<p>How do I just get it to temp without running a print job?</p>]]></content>
			<author>
				<name><![CDATA[hansen644]]></name>
				<uri>https://www.soliforum.com/user/7268/</uri>
			</author>
			<updated>2015-01-31T13:44:48Z</updated>
			<id>https://www.soliforum.com/post/82554/#p82554</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Proper way to change filament in repetier host?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/82154/#p82154" />
			<content type="html"><![CDATA[<p>Ok thank you very much.</p>]]></content>
			<author>
				<name><![CDATA[hansen644]]></name>
				<uri>https://www.soliforum.com/user/7268/</uri>
			</author>
			<updated>2015-01-29T02:44:42Z</updated>
			<id>https://www.soliforum.com/post/82154/#p82154</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Proper way to change filament in repetier host?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/81919/#p81919" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>hansen644 wrote:</cite><blockquote><p>New to repetier host here. How do I change my filament?&nbsp; Is there a correct way?</p></blockquote></div><p>Connect to the printer, go to manual tab, heat extruder to set temp. Once heated use manual extrude button at 100mm in reverse, or just use the release lever on the head and pull the filament out. The main thing is to make sure it is at full temp.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-01-27T21:29:33Z</updated>
			<id>https://www.soliforum.com/post/81919/#p81919</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Proper way to change filament in repetier host?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/81916/#p81916" />
			<content type="html"><![CDATA[<p>New to repetier host here. How do I change my filament?&nbsp; Is there a correct way?</p>]]></content>
			<author>
				<name><![CDATA[hansen644]]></name>
				<uri>https://www.soliforum.com/user/7268/</uri>
			</author>
			<updated>2015-01-27T21:12:11Z</updated>
			<id>https://www.soliforum.com/post/81916/#p81916</id>
		</entry>
</feed>