	<title type="html"><![CDATA[SoliForum - 3D Printing Community — PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/9529/" />
	<updated>2015-02-07T11:47:48Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/9529/pla-print-fan-for-20a-working-progress-for-curling-on-overhangs/</id>
		<entry>
			<title type="html"><![CDATA[Re: PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83850/#p83850" />
			<content type="html"><![CDATA[<p>Ok the fan it&#039;s finished</p><p><a href="http://www.thingiverse.com/thing:671135">http://www.thingiverse.com/thing:671135</a></p><p>This is my 80cm fan cooler for PLA printing. Specially for difficult prints that have overhangs, without a fan I wasn&#039;t able to keep the curlings out. Prior this I used a fan on the side but the air didn&#039;t reach evenly.</p><p>I used a 80cm fan, because that&#039;s what I got in hand. I had it usb connected directly to the printer, but I turned on after the 3-4 first layers, specially if they are the brim/rafts.</p><p>Print it on ABS (because the heat too close to the nozzles) and to avoid hard-to-remove supports, print it on slic3r/simplify3d at 90 degress (stl it&#039;s already rotated), so you don&#039;t get any supports inside the air-exit. If you print it flat you might have problems removing the supports.</p><p>Remember to keep the door open since it&#039;s the only area that it will hit.</p><p>The clip and fan have a really nice grip, on fast prints it stays put, but if there&#039;s too much x-y shake, it might move, it shouldn&#039;t.</p><p>Use it at your own risk.</p><p>The design it&#039;s inspired from <a href="http://www.thingiverse.com/thing:553792">http://www.thingiverse.com/thing:553792</a> by mordiev, but the measures and clip holder didn&#039;t did it for me so I have to start from the scratch.</p><p>Note: Both parts do &#039;clip&#039; ok, but if you are going to print with it, please glue both parts to avoid surprises.</p><p>Extra note: I wont be improving this, since in a week or two I&#039;ll have an Ultimaker. If anyone on europe it&#039;s interested on my DaVinci 2.0A (no more than 60h printing time) for a really special sale price, just send me a msg.</p>]]></content>
			<author>
				<name><![CDATA[Neotko]]></name>
				<uri>https://www.soliforum.com/user/8233/</uri>
			</author>
			<updated>2015-02-07T11:47:48Z</updated>
			<id>https://www.soliforum.com/post/83850/#p83850</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/83013/#p83013" />
			<content type="html"><![CDATA[<p>Well the design has 2 flaws. 1st the air does not point directly on the nozzle printed area (mistake measuring) and 2nd. The union of both parts it&#039;s a bit thin and it breaks easy if you don&#039;t remove it correctly, a bit of glue could fix that.</p><p>So, for the final design I&#039;ll:<br />- Make 40-50cm size for others fans. (this design it&#039;s for one fan I&#039;m gonna use of 80cm)<br />- Improve the union of both parts so it&#039;s harder to break.</p><p>Here some photos of the final print, as planned the support its minimum and it printed quite nicely at 0.3, a bit of warp on the 0.3 wall size since this is printed on ABS so it can hold better the heat (PLA might melt). Also this might melt... Who knows I need to test it XD. At the worse case scenario this would make a really great fan since it grabs to the metal bars and behind the connectors so it might have very little or zero &#039;movement&#039; while printing.</p><p>Next post, the final stage and some PLA printing with / without.</p>]]></content>
			<author>
				<name><![CDATA[Neotko]]></name>
				<uri>https://www.soliforum.com/user/8233/</uri>
			</author>
			<updated>2015-02-03T15:14:11Z</updated>
			<id>https://www.soliforum.com/post/83013/#p83013</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/82942/#p82942" />
			<content type="html"><![CDATA[<p>Great progress.&nbsp; Can&#039;t wait to see some example prints.</p><p>Have you done any other mods to print PLA?&nbsp; Are you successfully printing PLA?</p><p>Thanks,</p>]]></content>
			<author>
				<name><![CDATA[Flyer007]]></name>
				<uri>https://www.soliforum.com/user/9229/</uri>
			</author>
			<updated>2015-02-03T01:34:48Z</updated>
			<id>https://www.soliforum.com/post/82942/#p82942</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/82909/#p82909" />
			<content type="html"><![CDATA[<p>Finally I was able to end the design. Next post will be to upload the stl and show some photos of it working</p><p>The part that was more challenging was to avoid support, and I was able to do cut the supports to a minimum, and more important the inside air exit has zero supports <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></content>
			<author>
				<name><![CDATA[Neotko]]></name>
				<uri>https://www.soliforum.com/user/8233/</uri>
			</author>
			<updated>2015-02-02T20:25:11Z</updated>
			<id>https://www.soliforum.com/post/82909/#p82909</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/82263/#p82263" />
			<content type="html"><![CDATA[<p>As for the supports issue, I&#039;ve generally found slic3r does a crap job on making easily removable supports.</p><p>Cura or CraftWare does a great job (as does S3D).&nbsp; CraftWare has S3D&#039;s customizable support feature.</p><br /><p>I recently made a bracket, and in the vertical direction it had a gap halfway up.&nbsp; &nbsp;Like this (the gap was part of a spool hanger on thingiverse, so I couldn&#039;t just flip it on its side):<br /></p><div class="codebox"><pre><code>====||
====||
====||
    ||
====||
====||</code></pre></div><p>Slic3r insisted on making an elaborate support structure to support the gap.&nbsp; Except this support structure was always too close to the bracket and would fuse with it (unless I printed extremely slow with a ridiculous cooling time).</p><p>CraftWare just printed a &quot;shim&quot; in a direction orthogonal to the &quot;grain&quot; of the gap.&nbsp; Essentially making an easily removable shim with few contact points.&nbsp; No elaborate support structure was needed.</p>]]></content>
			<author>
				<name><![CDATA[jnadke]]></name>
				<uri>https://www.soliforum.com/user/9208/</uri>
			</author>
			<updated>2015-01-29T17:58:27Z</updated>
			<id>https://www.soliforum.com/post/82263/#p82263</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/82075/#p82075" />
			<content type="html"><![CDATA[<p>I will. This week it&#039;s very complicated because of work. But this weekend I wan&#039;t to road test it and start with the final design to upload it.</p>]]></content>
			<author>
				<name><![CDATA[Neotko]]></name>
				<uri>https://www.soliforum.com/user/8233/</uri>
			</author>
			<updated>2015-01-28T19:19:35Z</updated>
			<id>https://www.soliforum.com/post/82075/#p82075</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/82068/#p82068" />
			<content type="html"><![CDATA[<p>Looks interesting.&nbsp; Would be great if you did some on and off print examples to show the real benefits.</p>]]></content>
			<author>
				<name><![CDATA[Flyer007]]></name>
				<uri>https://www.soliforum.com/user/9229/</uri>
			</author>
			<updated>2015-01-28T18:39:42Z</updated>
			<id>https://www.soliforum.com/post/82068/#p82068</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[PLA print fan for 2.0A (working progress) for Curling on overhangs]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/81768/#p81768" />
			<content type="html"><![CDATA[<p>I wanted to share my fan head mount for the duo 2.0A. It&#039;s designed to cool the printed pla (not the heads). I started the designs looking at one duo fan holder for duo 2 that&#039;s on thingiverse (thing:553792) but I started from the scrach and tookmy own meassures since I&#039;m using a heavy 8x8cm fan conected via usb. Remember this fan isnt to cool the hot end, it&#039;s to avoid curling on overhangs and make the placool down faster. For rectangular design isn&#039;t needed but for the stuff I&#039;m working (wood pla with a lot of overhangs) it&#039;s a must for me. </p><p>Also this it&#039;s a beta. I&#039;ll post the files on thingiverse this weekend after I make a few ajustments.</p><p>My fan box:<br />- Hangs to the motors and gets a little grip arround side connectors (not cables)<br />- Pass though the space of the rails. <br />- Can hold a &#039;heavy&#039; fan without problem. <br />- Get&#039;s the grip of the metal of the x and doesn&#039;t hit on sides so the extruder moves freely. </p><p>Problems so far:<br />- The supports inside the fan are hard to remove, but easy if printed with S3D.<br />- The front door must stay open. It&#039;s the only area where it &#039;hits&#039;. <br />- I needto test it futher on &#039;shaky&#039; prints.</p>]]></content>
			<author>
				<name><![CDATA[Neotko]]></name>
				<uri>https://www.soliforum.com/user/8233/</uri>
			</author>
			<updated>2015-01-27T01:09:53Z</updated>
			<id>https://www.soliforum.com/post/81768/#p81768</id>
		</entry>