			<title type="html"><![CDATA[Re: 0031 fault]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/81913/#p81913" />
			<content type="html"><![CDATA[<p>I had this issue. It also showed 0031 on occasion.</p><p>When facing the printer, on the right side of the extruder is some sort of sensor / plug that goes into the extruder. This appeared to becoming loose when printing.</p><p>It wouldn&#039;t cause and issue when printing, but once finished, it wouldn&#039;t return to the correct home axis and do its cleaning motion etc in the middle.</p><p>I had to push this sensor back in stiff a few times and it hasn&#039;t happened for a while now.</p>]]></content>
			<author>
				<name><![CDATA[Gee]]></name>
				<uri>https://www.soliforum.com/user/7787/</uri>
			</author>
			<updated>2015-01-27T21:03:26Z</updated>
			<id>https://www.soliforum.com/post/81913/#p81913</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: 0031 fault]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/81544/#p81544" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>bill wrote:</cite><blockquote><p>Brandnew machine shows 0031 fault no idea how to rectify handbook useless</p></blockquote></div><p>A google search for that error tells you that the machine does not see the Y home sensor functioning correctly. Make sure the harness is plugged in well to it. If the is a 1.0 or 1.0A then that sensor is the white part in the upper back left corner.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-01-26T01:02:23Z</updated>
			<id>https://www.soliforum.com/post/81544/#p81544</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[0031 fault]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/81523/#p81523" />
			<content type="html"><![CDATA[<p>Brandnew machine shows 0031 fault no idea how to rectify handbook useless</p>]]></content>
			<author>
				<name><![CDATA[bill]]></name>
				<uri>https://www.soliforum.com/user/9020/</uri>
			</author>
			<updated>2015-01-25T22:59:06Z</updated>
			<id>https://www.soliforum.com/post/81523/#p81523</id>