			<title type="html"><![CDATA[Re: sticking to bed help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/78357/#p78357" />
			<content type="html"><![CDATA[<p>I have a chip resetter from wctek</p>]]></content>
			<author>
				<name><![CDATA[hansen644]]></name>
				<uri>https://www.soliforum.com/user/7268/</uri>
			</author>
			<updated>2015-01-10T16:32:48Z</updated>
			<id>https://www.soliforum.com/post/78357/#p78357</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: sticking to bed help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/78354/#p78354" />
			<content type="html"><![CDATA[<p>If you have stock soft/firmware, how are you changing the temps?</p>]]></content>
			<author>
				<name><![CDATA[tonyno]]></name>
				<uri>https://www.soliforum.com/user/8582/</uri>
			</author>
			<updated>2015-01-10T16:05:13Z</updated>
			<id>https://www.soliforum.com/post/78354/#p78354</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: sticking to bed help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/78328/#p78328" />
			<content type="html"><![CDATA[<p>I would not go above 120. Its more about the beds ABS substructure than the actual heater.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-01-10T04:42:56Z</updated>
			<id>https://www.soliforum.com/post/78328/#p78328</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: sticking to bed help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/78323/#p78323" />
			<content type="html"><![CDATA[<p>ok thanks. what is the max temp I can set the bed at and be safe it will not damage the bed heater?</p>]]></content>
			<author>
				<name><![CDATA[hansen644]]></name>
				<uri>https://www.soliforum.com/user/7268/</uri>
			</author>
			<updated>2015-01-10T04:22:45Z</updated>
			<id>https://www.soliforum.com/post/78323/#p78323</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: sticking to bed help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/78322/#p78322" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>hansen644 wrote:</cite><blockquote><p>Hi I am trying to print a quadcopter and its edges go all the way to the edges of the bed. Can not seem to get the front left corner layers to stay stuck to the bed after a few layers it warps up. I have bed temp set at 106 and filament 225. I have tried glue and also hairspray on the bed with no luck. Also have tried making up some abs slurry but same problem and also tired printing it on a raft and the raft also does the same thing in that area.</p></blockquote></div><p>Try a higher bed temp. I never use less than 110 and most of the time 115.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-01-10T04:11:04Z</updated>
			<id>https://www.soliforum.com/post/78322/#p78322</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: sticking to bed help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/78321/#p78321" />
			<content type="html"><![CDATA[<p>Note: I am using Stock xyz firm and software.</p>]]></content>
			<author>
				<name><![CDATA[hansen644]]></name>
				<uri>https://www.soliforum.com/user/7268/</uri>
			</author>
			<updated>2015-01-10T04:10:39Z</updated>
			<id>https://www.soliforum.com/post/78321/#p78321</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[sticking to bed help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/78320/#p78320" />
			<content type="html"><![CDATA[<p>Hi I am trying to print a quadcopter and its edges go all the way to the edges of the bed. Can not seem to get the front left corner layers to stay stuck to the bed after a few layers it warps up. I have bed temp set at 106 and filament 225. I have tried glue and also hairspray on the bed with no luck. Also have tried making up some abs slurry but same problem and also tired printing it on a raft and the raft also does the same thing in that area.</p>]]></content>
			<author>
				<name><![CDATA[hansen644]]></name>
				<uri>https://www.soliforum.com/user/7268/</uri>
			</author>
			<updated>2015-01-10T04:09:53Z</updated>
			<id>https://www.soliforum.com/post/78320/#p78320</id>
		</entry>