			<title type="html"><![CDATA[Re: Skeinforge configuration]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/7538/#p7538" />
			<content type="html"><![CDATA[<p>Thanks!</p>]]></content>
			<author>
				<name><![CDATA[perlguy]]></name>
				<uri>https://www.soliforum.com/user/142/</uri>
			</author>
			<updated>2012-12-19T22:02:16Z</updated>
			<id>https://www.soliforum.com/post/7538/#p7538</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Skeinforge configuration]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/7521/#p7521" />
			<content type="html"><![CDATA[<p>On the analyze tab, uncheck &quot;activate skeiniso&quot;</p>]]></content>
			<author>
				<name><![CDATA[cmetzel]]></name>
				<uri>https://www.soliforum.com/user/78/</uri>
			</author>
			<updated>2012-12-19T18:52:28Z</updated>
			<id>https://www.soliforum.com/post/7521/#p7521</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Skeinforge configuration]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/7518/#p7518" />
			<content type="html"><![CDATA[<p>I was wondering if anyone knew off-hand what the setting is that pops up the window with the object print diagram when skeinforge has finished processing an STL file into gcode.&nbsp; I would like to turn off that feature, but so far have not been able to figure out where in the settings it is.</p><p>Thanks!</p>]]></content>
			<author>
				<name><![CDATA[perlguy]]></name>
				<uri>https://www.soliforum.com/user/142/</uri>
			</author>
			<updated>2012-12-19T18:09:20Z</updated>
			<id>https://www.soliforum.com/post/7518/#p7518</id>
		</entry>
</feed>