<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — metal filaments.]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/8249/" />
	<updated>2014-12-03T23:28:22Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/8249/metal-filaments/</id>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/73901/#p73901" />
			<content type="html"><![CDATA[<p>Proto-pasta is releasing stainless steel/pla and magnetic iron/pla soon.</p>]]></content>
			<author>
				<name><![CDATA[AndersE]]></name>
				<uri>https://www.soliforum.com/user/6609/</uri>
			</author>
			<updated>2014-12-03T23:28:22Z</updated>
			<id>https://www.soliforum.com/post/73901/#p73901</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/73294/#p73294" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>frozensoda wrote:</cite><blockquote><p>I work for a steel and aluminium company, I have access to powdered aluminium and iron oxide for free(in small quantities, and yes it&#039;s allowed I&#039;m no thief <img src="https://www.soliforum.com/img/smilies/tongue.png" width="15" height="15" alt="tongue" />) if anyone is interested in trying aluminium or iron oxide, let me know and I&#039;ll work out shipping some to you.</p></blockquote></div><p>Careful not to mix those two... <a href="http://en.wikipedia.org/wiki/Thermite">http://en.wikipedia.org/wiki/Thermite</a></p>]]></content>
			<author>
				<name><![CDATA[grob]]></name>
				<uri>https://www.soliforum.com/user/4515/</uri>
			</author>
			<updated>2014-11-28T03:09:05Z</updated>
			<id>https://www.soliforum.com/post/73294/#p73294</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71295/#p71295" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>elmoret wrote:</cite><blockquote><p>The store credit for filament reviews policy is stickied in the DIY filament forum.</p></blockquote></div><p>sorry</p>]]></content>
			<author>
				<name><![CDATA[frozensoda]]></name>
				<uri>https://www.soliforum.com/user/738/</uri>
			</author>
			<updated>2014-11-09T03:19:07Z</updated>
			<id>https://www.soliforum.com/post/71295/#p71295</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71292/#p71292" />
			<content type="html"><![CDATA[<p>The store credit for filament reviews policy is stickied in the DIY filament forum.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2014-11-09T03:02:07Z</updated>
			<id>https://www.soliforum.com/post/71292/#p71292</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71291/#p71291" />
			<content type="html"><![CDATA[<p>I work for a steel and aluminium company, I have access to powdered aluminium and iron oxide for free(in small quantities, and yes it&#039;s allowed I&#039;m no thief <img src="https://www.soliforum.com/img/smilies/tongue.png" width="15" height="15" alt="tongue" />) if anyone is interested in trying aluminium or iron oxide, let me know and I&#039;ll work out shipping some to you. Also, elmoret, we spoke briefly before about me purchasing a filastruder for a discount if I test new materials, would this count? In feburary I&#039;m expecting a tidy sum from my tax refund so I will definitely be buying one either way but I&#039;d love to get the discount.</p>]]></content>
			<author>
				<name><![CDATA[frozensoda]]></name>
				<uri>https://www.soliforum.com/user/738/</uri>
			</author>
			<updated>2014-11-09T02:44:48Z</updated>
			<id>https://www.soliforum.com/post/71291/#p71291</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71270/#p71270" />
			<content type="html"><![CDATA[<p>saltlakemetals&nbsp; sells powered metals, relatively affordable. its a pricy project: lets hope it works.</p>]]></content>
			<author>
				<name><![CDATA[pistar]]></name>
				<uri>https://www.soliforum.com/user/7979/</uri>
			</author>
			<updated>2014-11-08T22:41:23Z</updated>
			<id>https://www.soliforum.com/post/71270/#p71270</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71269/#p71269" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>pistar wrote:</cite><blockquote><p>low might be a little of a stench but its 80% by weight meaning it might only be 5% by volume. I&#039;m curious to know the volume of bronze to PLA in the bronzefill.</p></blockquote></div><p>Volume doesn&#039;t matter, mass does.</p><p>1000 grams of bronzefill is 800 grams of bronze.</p><p>That&#039;s $400 of silver assuming you can get it at spot prices, and that&#039;s before you&#039;ve paid to have it powdered. </p><p>The powdering isn&#039;t cheap either, here&#039;s 100 grams for $320:</p><p><a href="http://www.saltlakemetals.com/Silver_Powder.htm">http://www.saltlakemetals.com/Silver_Powder.htm</a></p><p>But don&#039;t let my shallow pockets dissuade you.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2014-11-08T22:34:03Z</updated>
			<id>https://www.soliforum.com/post/71269/#p71269</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71265/#p71265" />
			<content type="html"><![CDATA[<p>low might be a little of a stench but its 80% by weight meaning it might only be 5% by volume. I&#039;m curious to know the volume of bronze to PLA in the bronzefill.</p>]]></content>
			<author>
				<name><![CDATA[pistar]]></name>
				<uri>https://www.soliforum.com/user/7979/</uri>
			</author>
			<updated>2014-11-08T22:02:45Z</updated>
			<id>https://www.soliforum.com/post/71265/#p71265</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71086/#p71086" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>pistar wrote:</cite><blockquote><p>i don&#039;t need a kilogram,&nbsp; the percentage of metal to plastic in the metal filament coming out is low. $100 in powdered silver will go a long way.</p></blockquote></div><p>Bronzefill is 80% bronze by weight. </p><p>I wouldn&#039;t call that &quot;low&quot;.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2014-11-07T13:56:18Z</updated>
			<id>https://www.soliforum.com/post/71086/#p71086</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71085/#p71085" />
			<content type="html"><![CDATA[<p>also, im not printing large things.</p>]]></content>
			<author>
				<name><![CDATA[pistar]]></name>
				<uri>https://www.soliforum.com/user/7979/</uri>
			</author>
			<updated>2014-11-07T13:53:57Z</updated>
			<id>https://www.soliforum.com/post/71085/#p71085</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71084/#p71084" />
			<content type="html"><![CDATA[<p>i don&#039;t need a kilogram,&nbsp; the percentage of metal to plastic in the metal filament coming out is low. $100 in powdered silver will go a long way.</p>]]></content>
			<author>
				<name><![CDATA[pistar]]></name>
				<uri>https://www.soliforum.com/user/7979/</uri>
			</author>
			<updated>2014-11-07T13:53:12Z</updated>
			<id>https://www.soliforum.com/post/71084/#p71084</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71024/#p71024" />
			<content type="html"><![CDATA[<p>It shouldn&#039;t damage the Filastruder (it may increase wear over the long term), but the bigger concern is how it is going to be extraordinarily expensive. Have you priced silver? A kilogram is well over $500, and that&#039;s before it is powdered.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2014-11-07T03:25:22Z</updated>
			<id>https://www.soliforum.com/post/71024/#p71024</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[metal filaments.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/71021/#p71021" />
			<content type="html"><![CDATA[<p>a few metal filaments have been coming out recently.&nbsp; &nbsp;I&#039;ve personally used the copper and the bronze filament and I&#039;ve seen theres also an aluminum one out now too. do you think the filastruder can handle any percent of powdered metal added to the pellet mix? I&#039;m dying to get my hands on some silver filament but i feel like making it myself will be the only way I&#039;m going to get it. what dod you think? powdered silver + abs pellets + filastruder = awesome silver (Ag) filament or dead filastruder ?</p>]]></content>
			<author>
				<name><![CDATA[pistar]]></name>
				<uri>https://www.soliforum.com/user/7979/</uri>
			</author>
			<updated>2014-11-07T03:11:40Z</updated>
			<id>https://www.soliforum.com/post/71021/#p71021</id>
		</entry>
</feed>