<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — ABS slurry works excellent!]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/7857/" />
	<updated>2014-09-30T18:06:04Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/7857/abs-slurry-works-excellent/</id>
		<entry>
			<title type="html"><![CDATA[Re: ABS slurry works excellent!]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/67363/#p67363" />
			<content type="html"><![CDATA[<p>Hey I was wondering how does ABS slurry work?</p>]]></content>
			<author>
				<name><![CDATA[cmetzel]]></name>
				<uri>https://www.soliforum.com/user/78/</uri>
			</author>
			<updated>2014-09-30T18:06:04Z</updated>
			<id>https://www.soliforum.com/post/67363/#p67363</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[ABS slurry works excellent!]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/67359/#p67359" />
			<content type="html"><![CDATA[<p>I had been using hairspray the past couple months to keep my pieces sticking. Yesterday for the first time I needed to make a fan for an electric motor that was about 6 inches wide and 2 tall, At first the hair spray wouldnt hold it, about mid print itd catch and ruin. Tried the abs slurry. Holy cow was i missing out. really helps rid of warping too but my goodness it works wonders. If you havent tried it, go do it now.</p>]]></content>
			<author>
				<name><![CDATA[shields1.as]]></name>
				<uri>https://www.soliforum.com/user/7171/</uri>
			</author>
			<updated>2014-09-30T16:44:35Z</updated>
			<id>https://www.soliforum.com/post/67359/#p67359</id>