			<title type="html"><![CDATA[Re: Cyrolite HiFlo made transparent filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/67192/#p67192" />
			<content type="html"><![CDATA[<p>Thats quite lots of airbubbles, super fail, as above mention dry your pellets. 5 Hour drying should do fine.</p>]]></content>
			<author>
				<name><![CDATA[oklok]]></name>
				<uri>https://www.soliforum.com/user/6232/</uri>
			</author>
			<updated>2014-09-27T13:21:27Z</updated>
			<id>https://www.soliforum.com/post/67192/#p67192</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Cyrolite HiFlo made transparent filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/67164/#p67164" />
			<content type="html"><![CDATA[<p>Good advice. Thank you sir !</p>]]></content>
			<author>
				<name><![CDATA[kszwab]]></name>
				<uri>https://www.soliforum.com/user/6745/</uri>
			</author>
			<updated>2014-09-27T00:00:52Z</updated>
			<id>https://www.soliforum.com/post/67164/#p67164</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Cyrolite HiFlo made transparent filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66984/#p66984" />
			<content type="html"><![CDATA[<p>Air bubbles indicate it was not sufficiently dried prior to extrusion.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2014-09-25T02:48:47Z</updated>
			<id>https://www.soliforum.com/post/66984/#p66984</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Cyrolite HiFlo made transparent filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66982/#p66982" />
			<content type="html"><![CDATA[<p>I scavenged some acryllic Cyrolite Hiflo pellets as in </p><p><a href="http://www.cyrolite.com/product/cyrolite-compounds/en/products/cyrolite/cyrolite-g20-hiflo/pages/default.aspx">http://www.cyrolite.com/product/cyrolit … fault.aspx</a></p><p>I managed to make excellent transparent filament using the filastruder using the extrusion temperature of 208C and inclination of 30 degrees on the filastruder.</p><p>Extrusion temperature on the Davinci at 250C, bed at 90C. Good adhesion using hairspray and glue, no clogging of the nozzle or any issues.</p><p>I can do a 1:100 colorant using some MG94 pale white or tan pellets to not confuse the optical sensor in the Davinci, although it works even without.</p><p>The occasional air bubbles do not make the filament brittle or create any issues with the prints.</p><p>Posting pictures soon and also review of the blue Cyrolite that looks like crystal meth from Breaking Bad.</p>]]></content>
			<author>
				<name><![CDATA[kszwab]]></name>
				<uri>https://www.soliforum.com/user/6745/</uri>
			</author>
			<updated>2014-09-25T01:56:25Z</updated>
			<id>https://www.soliforum.com/post/66982/#p66982</id>
		</entry>
</feed>