	<title type="html"><![CDATA[SoliForum - 3D Printing Community — adding colors to the filament?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/7764/" />
	<updated>2014-09-23T07:15:33Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/7764/adding-colors-to-the-filament/</id>
		<entry>
			<title type="html"><![CDATA[Re: adding colors to the filament?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66814/#p66814" />
			<content type="html"><![CDATA[<p>You need to track down local polymer suppliers.&nbsp; If you can find a factory that makes plastic injection moulded items they might be able to point you to a supplier.</p><p>As you only use 1% of colour, it is not very expensive to ship, especially if you buy a number of basic colours.&nbsp; This is the reason why I originally chose to include black,white,yellow, red, blue in a selection as you can make most colours by mixing these.</p><p>Most commercial suppliers want you to buy a minimum of 1kg or 5kg of each colour which would last you years (unless you are VERY prolific at making filament.</p>]]></content>
			<author>
				<name><![CDATA[CraigRK]]></name>
				<uri>https://www.soliforum.com/user/1188/</uri>
			</author>
			<updated>2014-09-23T07:15:33Z</updated>
			<id>https://www.soliforum.com/post/66814/#p66814</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: adding colors to the filament?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66728/#p66728" />
			<content type="html"><![CDATA[<p>Thanks.<br />Any ideas where to get them in Georgia? I dont know how its called in georgian or russian. If it has other uses maybe I could buy it locally in corresponding shop and not have to ship it every time.</p>]]></content>
			<author>
				<name><![CDATA[a3393341]]></name>
				<uri>https://www.soliforum.com/user/7392/</uri>
			</author>
			<updated>2014-09-22T21:10:46Z</updated>
			<id>https://www.soliforum.com/post/66728/#p66728</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: adding colors to the filament?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66646/#p66646" />
			<content type="html"><![CDATA[<p>You need Masterbatch</p><p>Have a look at the &quot;Polymers&quot; sticky at the top of the forum: <a href="http://www.soliforum.com/topic/4195/polymer-suppliers/">http://www.soliforum.com/topic/4195/polymer-suppliers/</a></p><p>And the &quot;Colorants&quot; topic: <a href="http://www.soliforum.com/topic/2123/colorants-masterbatch/">http://www.soliforum.com/topic/2123/col … sterbatch/</a></p><p>Regards,<br />Craig</p>]]></content>
			<author>
				<name><![CDATA[CraigRK]]></name>
				<uri>https://www.soliforum.com/user/1188/</uri>
			</author>
			<updated>2014-09-22T09:09:00Z</updated>
			<id>https://www.soliforum.com/post/66646/#p66646</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[adding colors to the filament?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66644/#p66644" />
			<content type="html"><![CDATA[<p>Im sorry if this has been asked several times already and I failed to use the search tool properly or find a page with an article about this.</p><p>I have natural color ABS pellets I&#039;d like to turn into filament when I get my Filastruder+Filawinder shipped.</p><p>What do I need to add to the pellets to get colored filament? Powder? Something else? What is it called, where can I get them and is there a page where I can learn from others experiences whats a good mix ratio of pellets and the colorants?</p><p>Thank you.</p>]]></content>
			<author>
				<name><![CDATA[a3393341]]></name>
				<uri>https://www.soliforum.com/user/7392/</uri>
			</author>
			<updated>2014-09-22T07:41:58Z</updated>
			<id>https://www.soliforum.com/post/66644/#p66644</id>