	<title type="html"><![CDATA[SoliForum - 3D Printing Community — New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/7708/" />
	<updated>2014-10-13T17:07:01Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/7708/new-filament-for-da-vinciprints-coming-out-thinner-stringy-stretchy/</id>
		<entry>
			<title type="html"><![CDATA[Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/68530/#p68530" />
			<content type="html"><![CDATA[<p>Wow, ok, thanks for all the recommendations, I will revert to firmware g, and adjust the tightness.</p><p>I appreciate it guys<br />Alex</p>]]></content>
			<author>
				<name><![CDATA[alexandernadeau]]></name>
				<uri>https://www.soliforum.com/user/7240/</uri>
			</author>
			<updated>2014-10-13T17:07:01Z</updated>
			<id>https://www.soliforum.com/post/68530/#p68530</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/68529/#p68529" />
			<content type="html"><![CDATA[<p>Looks like a typical problem with firmware J.<br />Revert back to firmware G should solve your problem</p>]]></content>
			<author>
				<name><![CDATA[yuyueyuyue]]></name>
				<uri>https://www.soliforum.com/user/7423/</uri>
			</author>
			<updated>2014-10-13T17:05:38Z</updated>
			<id>https://www.soliforum.com/post/68529/#p68529</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/68521/#p68521" />
			<content type="html"><![CDATA[<p>What version of software and firmware are you running.&nbsp; This looks to me to be a non-filament based issue.&nbsp; Also verify your belts have the proper tension.&nbsp; My printer was missing the screw on the X-Axis that locks it into place when I got it, which was causing some issues like this only not nearly as severe.</p>]]></content>
			<author>
				<name><![CDATA[Jaeg]]></name>
				<uri>https://www.soliforum.com/user/2008/</uri>
			</author>
			<updated>2014-10-13T15:49:23Z</updated>
			<id>https://www.soliforum.com/post/68521/#p68521</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/68400/#p68400" />
			<content type="html"><![CDATA[<p>I have purchased three other types of filament, and they beleive its a problem wth the extruder multiplier. I&#039;m going to try to screw with it after canadian thanksgiving.</p>]]></content>
			<author>
				<name><![CDATA[alexandernadeau]]></name>
				<uri>https://www.soliforum.com/user/7240/</uri>
			</author>
			<updated>2014-10-12T00:47:14Z</updated>
			<id>https://www.soliforum.com/post/68400/#p68400</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/68396/#p68396" />
			<content type="html"><![CDATA[<p>just checking here to see if this issue was ever resolved? I am having th EXACT same problem right now only i am using the hatchbox ABS filament. </p><p>My printers are almost spongy</p>]]></content>
			<author>
				<name><![CDATA[darin.prater]]></name>
				<uri>https://www.soliforum.com/user/7653/</uri>
			</author>
			<updated>2014-10-12T00:41:11Z</updated>
			<id>https://www.soliforum.com/post/68396/#p68396</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66949/#p66949" />
			<content type="html"><![CDATA[<p>What temperatures are you using? So far I&#039;ve had better luck running non-XYZ filament with a higher temperature than the stock cartridge calls for. I think the default is 210, Currently I&#039;m running at 230C with the heated bed at 115 with kapton to prevent warping.</p><p>Also on a side note, check to make sure your belts are tight, and that you do not have any cracked pulleys!</p>]]></content>
			<author>
				<name><![CDATA[mechpw]]></name>
				<uri>https://www.soliforum.com/user/7446/</uri>
			</author>
			<updated>2014-09-24T14:39:30Z</updated>
			<id>https://www.soliforum.com/post/66949/#p66949</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66342/#p66342" />
			<content type="html"><![CDATA[<p>I&#039;m using a resetter and had the same problem, see the topic &#039;filament-coming-out-blotchy&#039; still on the front page of the forum for XYZ Printing DaVinci</p><p>I got it to work for a while, then had to disassemble my extruder head to clean it (Not sure if the need to clean was related or if it was my homemade filament)</p>]]></content>
			<author>
				<name><![CDATA[jack.kleinman]]></name>
				<uri>https://www.soliforum.com/user/7186/</uri>
			</author>
			<updated>2014-09-18T02:20:57Z</updated>
			<id>https://www.soliforum.com/post/66342/#p66342</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[New filament for da vinci,Prints coming out thinner, stringy, stretchy]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/66335/#p66335" />
			<content type="html"><![CDATA[<p>hey guys, </p><p>I changed filament today with a cartridge resetter.... I am now using boots industries top notch filament, which is 1.75mm white abs. when I made a test print, the print came out very stringy, barely infilled, and separated from each layer, making it almost stretchy. does anyone know what settings I would have to change in slic3r to make this new filament work like the xyzprinting cartridge work, which was a lot better?</p><p>heres some pics:</p><p>First picture shows new filament on the left, xyz on right.</p><p>Thanks<br />Alex</p>]]></content>
			<author>
				<name><![CDATA[alexandernadeau]]></name>
				<uri>https://www.soliforum.com/user/7240/</uri>
			</author>
			<updated>2014-09-18T00:21:35Z</updated>
			<id>https://www.soliforum.com/post/66335/#p66335</id>
		</entry>
</feed>