<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — ColorFabb XT]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/7371/" />
	<updated>2014-08-18T14:34:41Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/7371/colorfabb-xt/</id>
		<entry>
			<title type="html"><![CDATA[Re: ColorFabb XT]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/63669/#p63669" />
			<content type="html"><![CDATA[<p>Note: I tried Acetone vapor smoothing and it did not work. I will try M.E.K Substiute vapor smoothing at some point (like I did for PLA) to see if that works.</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-08-18T14:34:41Z</updated>
			<id>https://www.soliforum.com/post/63669/#p63669</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[ColorFabb XT]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/63668/#p63668" />
			<content type="html"><![CDATA[<p>I have begun to play with some ColorFabb XT copolyester ( <a href="http://colorfabb.com/xt-copolyester">http://colorfabb.com/xt-copolyester</a> ). So far I like it. It is pretty transparent and seems strong and reminds me of Nylon or T-glase, but not exactly.</p><p>The Settings I have used:</p><p>- Hotend Temperature of 257 (on E3D hotend)<br />- Bed temp of 70 degrees<br />- I find that at 85% speed it stuck a little better on sharper corners, but that was a minor issue. And maybe that can even be fixed with a lil higher temperatures and further tweeks<br />- For the first layer I found it sticks better if I drop the speed to 50-60% for the first layer.</p><p>I had no issues printing with this stuff and it is fairly transparent and nicely luminescent. Easy to add good looking color accents with magic marker too like I did with the heart pendent.</p><p><span class="postimg"><img src="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=6032&amp;download=0" alt="http://www.soliforum.com/misc.php?action=pun_attachment&amp;amp;item=6032&amp;amp;download=0" /></span><br /><span class="postimg"><img src="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=6031&amp;download=0" alt="http://www.soliforum.com/misc.php?action=pun_attachment&amp;amp;item=6031&amp;amp;download=0" /></span></p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-08-18T14:26:00Z</updated>
			<id>https://www.soliforum.com/post/63668/#p63668</id>
		</entry>
</feed>