<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Stellar Labs ABS Filament]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/7362/" />
	<updated>2014-09-08T21:46:09Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/7362/stellar-labs-abs-filament/</id>
		<entry>
			<title type="html"><![CDATA[Re: Stellar Labs ABS Filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/65784/#p65784" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>oklok wrote:</cite><blockquote><p>Thats kind of sucky to babsit your spool. Try to put something above the spool holder so it does not flap when reaching the end of it.</p></blockquote></div><p>That&#039;s a good idea.</p>]]></content>
			<author>
				<name><![CDATA[hairu526]]></name>
				<uri>https://www.soliforum.com/user/4789/</uri>
			</author>
			<updated>2014-09-08T21:46:09Z</updated>
			<id>https://www.soliforum.com/post/65784/#p65784</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Stellar Labs ABS Filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/65659/#p65659" />
			<content type="html"><![CDATA[<p>Thats kind of sucky to babsit your spool. Try to put something above the spool holder so it does not flap when reaching the end of it.</p>]]></content>
			<author>
				<name><![CDATA[oklok]]></name>
				<uri>https://www.soliforum.com/user/6232/</uri>
			</author>
			<updated>2014-09-07T06:39:39Z</updated>
			<id>https://www.soliforum.com/post/65659/#p65659</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Stellar Labs ABS Filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/65583/#p65583" />
			<content type="html"><![CDATA[<p>I&#039;m about halfway through the spool and it&#039;s been working pretty good for me.&nbsp; It sticks well and the diameter is consistent.&nbsp; The only issue is that the filament comes off the spool pretty easily and gets stuck on the spool holder until you use about 10%, so you have to babysit it until then.&nbsp; I&#039;m printing with the fairly normal temp of 215C extruder and 110C bed on SD2 with kapton over aluminum.</p>]]></content>
			<author>
				<name><![CDATA[hairu526]]></name>
				<uri>https://www.soliforum.com/user/4789/</uri>
			</author>
			<updated>2014-09-06T12:56:01Z</updated>
			<id>https://www.soliforum.com/post/65583/#p65583</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Stellar Labs ABS Filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/63574/#p63574" />
			<content type="html"><![CDATA[<p>Has anyone tried the Stellar Labs ABS Filament yet?</p><p><a href="http://www.mcmelectronics.com/product/310-0128">http://www.mcmelectronics.com/product/310-0128</a></p><p>It would be nice to have a table of filament from different manufacturers and info on how well they work with the Solidoodle and other printers along with the basic settings for best results....</p>]]></content>
			<author>
				<name><![CDATA[hairu526]]></name>
				<uri>https://www.soliforum.com/user/4789/</uri>
			</author>
			<updated>2014-08-17T14:06:04Z</updated>
			<id>https://www.soliforum.com/post/63574/#p63574</id>
		</entry>
</feed>