			<title type="html"><![CDATA[Re: TPE]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/61410/#p61410" />
			<content type="html"><![CDATA[<p>3m Multi-flex extrudes really great, but it has so much flex that i haven&#039;t been able to get it to print, I tried a 1/2abs 1/2multiflex and it worked but flex wasn&#039;t really there, but had a neat texture. I have 10lbs of it left so i&#039;m going to try some more mixing this week to test my new equipment.<br />I&#039;ll post results here<br />out of abs but have some pla&#039;s and pc and a few other things to try as well</p>]]></content>
			<author>
				<name><![CDATA[cor5151]]></name>
				<uri>https://www.soliforum.com/user/6072/</uri>
			</author>
			<updated>2014-07-29T08:04:56Z</updated>
			<id>https://www.soliforum.com/post/61410/#p61410</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[TPE]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/61395/#p61395" />
			<content type="html"><![CDATA[<p>Hey guys, I&#039;m new to the wide world of making your own filament as I&#039;ve only ever made ABS in my machine however I really want to play around with flexible filaments, would this be a good bet to try to extrude? </p><p><a href="http://cgi.ebay.com/ws/eBayISAPI.dll?ViewItem&amp;item=121100835310&amp;ssPageName=ADME:L:OC:US:3160">http://cgi.ebay.com/ws/eBayISAPI.dll?Vi … OC:US:3160</a></p><p>Any tips would be great too! Thanks again!</p>]]></content>
			<author>
				<name><![CDATA[michaudtime]]></name>
				<uri>https://www.soliforum.com/user/3726/</uri>
			</author>
			<updated>2014-07-29T02:22:42Z</updated>
			<id>https://www.soliforum.com/post/61395/#p61395</id>
		</entry>
</feed>