			<title type="html"><![CDATA[Re: print PP]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/59505/#p59505" />
			<content type="html"><![CDATA[<p>Hello JG,</p><p>Pls try nozzle as 250-280℃, and bed increased to 120-150℃. We sell PP filament also, and this is our parameter, maybe you can try it. Hope it can help you.</p><p>Best Regards,<br />Grace (grace@siridiwh.com)</p>]]></content>
			<author>
				<name><![CDATA[grace_siridi]]></name>
				<uri>https://www.soliforum.com/user/6374/</uri>
			</author>
			<updated>2014-06-30T03:10:33Z</updated>
			<id>https://www.soliforum.com/post/59505/#p59505</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: print PP]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/59504/#p59504" />
			<content type="html"><![CDATA[<p>Hello JG,</p><p>Pls try nozzle as 250-280℃, and bed increased to 120-150℃. We sell PP filament also, and this is our parameter, maybe you can try it. Hope it can help you.</p><p>Best Regards,<br />Grace (grace@siridiwh.com)</p>]]></content>
			<author>
				<name><![CDATA[grace_siridi]]></name>
				<uri>https://www.soliforum.com/user/6374/</uri>
			</author>
			<updated>2014-06-30T03:10:08Z</updated>
			<id>https://www.soliforum.com/post/59504/#p59504</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[print PP]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/58983/#p58983" />
			<content type="html"><![CDATA[<p>Hi,<br />I am trying to print a PP filament in our 3d printer. We have no adhesion to the bed, using 230ºC in the nozzle and the bed at 80ºC. We also used some lacquer or harispray in order to get a good adhesion, but.... it seems impossible!!! <br />Please, any recommendation? <br />Thanks in advance.<br />Kind regards,<br />JG</p>]]></content>
			<author>
				<name><![CDATA[jgoikoetxea]]></name>
				<uri>https://www.soliforum.com/user/6266/</uri>
			</author>
			<updated>2014-06-20T06:35:18Z</updated>
			<id>https://www.soliforum.com/post/58983/#p58983</id>
		</entry>
</feed>