			<title type="html"><![CDATA[Re: Hot melt filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/57288/#p57288" />
			<content type="html"><![CDATA[<p>TPE! I used duraflex, worked well in the Filastruder. Never tried printing it.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2014-05-29T14:02:02Z</updated>
			<id>https://www.soliforum.com/post/57288/#p57288</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Hot melt filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/57286/#p57286" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>Sungod3000 wrote:</cite><blockquote><p>but for what would you use it? Printing in hotglue?</p></blockquote></div><p>The use case would be to create rubbery/flexible parts.</p>]]></content>
			<author>
				<name><![CDATA[jesse]]></name>
				<uri>https://www.soliforum.com/user/1984/</uri>
			</author>
			<updated>2014-05-29T13:53:34Z</updated>
			<id>https://www.soliforum.com/post/57286/#p57286</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Hot melt filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/57269/#p57269" />
			<content type="html"><![CDATA[<p>Well cant be worse than PLA <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /> if you lower the temp down to 60-80C, but for what would you use it? Printing in hotglue?</p>]]></content>
			<author>
				<name><![CDATA[Sungod3000]]></name>
				<uri>https://www.soliforum.com/user/5754/</uri>
			</author>
			<updated>2014-05-29T10:26:21Z</updated>
			<id>https://www.soliforum.com/post/57269/#p57269</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Hot melt filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/56558/#p56558" />
			<content type="html"><![CDATA[<p>Has anyone tried making filament out of hot glue gun pellets?</p><p>For instance: <a href="http://www.ebay.com/itm/Hot-Melt-Glue-Pellets-Five-Pounds-/191180706020">http://www.ebay.com/itm/Hot-Melt-Glue-P … 1180706020</a></p>]]></content>
			<author>
				<name><![CDATA[jesse]]></name>
				<uri>https://www.soliforum.com/user/1984/</uri>
			</author>
			<updated>2014-05-18T20:51:30Z</updated>
			<id>https://www.soliforum.com/post/56558/#p56558</id>
		</entry>
</feed>