			<title type="html"><![CDATA[Re: Problems with circles]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55762/#p55762" />
			<content type="html"><![CDATA[<p>There is the stock fan on my printer (SD2), it seems to be going at all times.</p><p>I have no adjusted my cooling print speed, so I can try that.</p><p>I&#039;ll check out the &quot;how to end circle problems forever&quot; about those Y belts. I also have not tightened the various belts in a long time, and I have been printing a lot. </p><p>Thanks for the help.</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-05-06T12:42:07Z</updated>
			<id>https://www.soliforum.com/post/55762/#p55762</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Problems with circles]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55743/#p55743" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>accusedmonk wrote:</cite><blockquote><p>Do you have a fan on your printer?&nbsp; If not it would help a lot with the small features/layer being printed to fast. Also, under the filament settings, change your cooling print speed to 20mm/s or so</p><p>As far as actual calibration, this tutorial should help you out quite a bit:<br /><a href="http://wiki.solidoodle.com/belt-adjustment">http://wiki.solidoodle.com/belt-adjustment</a></p></blockquote></div><p>+1 I would add that circle problems are mostly caused by misalignment of the side Y-axis belts.&nbsp; Second to that is deflection of the y-axis drive rod.&nbsp; This can be fixed by adding a pillow block with bearings on that drive rod.&nbsp; Search &quot; how to end circle problems forever&quot;</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-05-06T02:43:35Z</updated>
			<id>https://www.soliforum.com/post/55743/#p55743</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Problems with circles]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55731/#p55731" />
			<content type="html"><![CDATA[<p>Do you have a fan on your printer?&nbsp; If not it would help a lot with the small features/layer being printed to fast. Also, under the filament settings, change your cooling print speed to 20mm/s or so</p><p>As far as actual calibration, this tutorial should help you out quite a bit:<br /><a href="http://wiki.solidoodle.com/belt-adjustment">http://wiki.solidoodle.com/belt-adjustment</a></p>]]></content>
			<author>
				<name><![CDATA[accusedmonk]]></name>
				<uri>https://www.soliforum.com/user/3772/</uri>
			</author>
			<updated>2014-05-06T01:22:55Z</updated>
			<id>https://www.soliforum.com/post/55731/#p55731</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Problems with circles]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55725/#p55725" />
			<content type="html"><![CDATA[<p>Seems my prints are ok except the worst part being circles and curves. Suggestions, I&#039;ve tried to calibrate what I can.</p>]]></content>
			<author>
				<name><![CDATA[LdyMox]]></name>
				<uri>https://www.soliforum.com/user/1758/</uri>
			</author>
			<updated>2014-05-06T00:23:46Z</updated>
			<id>https://www.soliforum.com/post/55725/#p55725</id>
		</entry>