			<title type="html"><![CDATA[Re: Silver Filament Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5664/#p5664" />
			<content type="html"><![CDATA[<p>I think Macmub is right. I am also using clear filament and temps are much different than pigmented ones...<br />If I set the extruder to 200c, the extrusion bubbles like crazy and it looks like the way it does in your pics.</p><p>I think in your case, the silver is actually silver colored particles(stuff?) mixed in with clear ABS and not pigmented ABS?... if that makes any sense... </p><p>And if that is the case, then the humidity and environment has a lot to do with how you should set the temperatures. I live in FL with pretty high humidity so I have to set my temps way low for my clear filament. Ive been printing .1mm at 175c and it&#039;s been working pretty well. You can almost see clearly through the prints as if it was injection molded. </p><p>You should definitely do as macmub suggested and write down and keep a record of all your settings. I think a good start is to watch the extruder as the temp rises and see what temp the filament becomes molten and ooses/bubbles out of the extruder (without you manually extruding.) Then try to stay close to that temperature range. Then just dial everything in from there. Took me a week but it&#039;s pretty sweet when things start to work.</p>]]></content>
			<author>
				<name><![CDATA[MeshMoth]]></name>
				<uri>https://www.soliforum.com/user/19/</uri>
			</author>
			<updated>2012-11-27T06:24:13Z</updated>
			<id>https://www.soliforum.com/post/5664/#p5664</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Silver Filament Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5640/#p5640" />
			<content type="html"><![CDATA[<p>Ive noticed different colors make for different prints. my black can be troublesome at high temps, also my clear is a real nightmare compared to my solid colors.</p><p>All just needs tweaking, Id suggest writing down your results for each color or type of filament so you have a reference should you run into problems down the line.</p>]]></content>
			<author>
				<name><![CDATA[macmub]]></name>
				<uri>https://www.soliforum.com/user/10/</uri>
			</author>
			<updated>2012-11-26T21:41:05Z</updated>
			<id>https://www.soliforum.com/post/5640/#p5640</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Silver Filament Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5603/#p5603" />
			<content type="html"><![CDATA[<p>Got a much improved print by lowering the temperate down to 185 and lowering the Extrusion Multiplier a little.</p>]]></content>
			<author>
				<name><![CDATA[caswal]]></name>
				<uri>https://www.soliforum.com/user/351/</uri>
			</author>
			<updated>2012-11-26T08:46:43Z</updated>
			<id>https://www.soliforum.com/post/5603/#p5603</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Silver Filament Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5601/#p5601" />
			<content type="html"><![CDATA[<p>Got some new silver filament in the mail today, but it is printing nowhere near the same quality level as the white abs that shipped with the SD.</p><p>First attempt, the perimeter is really blobby, was printed at 200 deg<br /><span class="postimg"><img src="https://lh5.googleusercontent.com/-EHItxOty8ww/ULMWJSYUa1I/AAAAAAAAAr4/64ske_6N-5M/s1024/IMG_4467.JPG" alt="https://lh5.googleusercontent.com/-EHItxOty8ww/ULMWJSYUa1I/AAAAAAAAAr4/64ske_6N-5M/s1024/IMG_4467.JPG" /></span></p><p>Dropped the temp by 10 down to 190, for the gear on the right:</p><p><span class="postimg"><img src="https://lh5.googleusercontent.com/-RSRHfeL6bIc/ULMWJE7JjjI/AAAAAAAAAr4/PGWxxc8vky0/s1024/IMG_4466.JPG" alt="https://lh5.googleusercontent.com/-RSRHfeL6bIc/ULMWJE7JjjI/AAAAAAAAAr4/PGWxxc8vky0/s1024/IMG_4466.JPG" /></span></p><p>It is somewhat better, but still quite rough. Is this just caused by printing too hot, or is the filament extrusion rate too fast as well? What would be really great is a guide (perhaps there is one and I don&#039;t know where it is). That has some pictures of common issues and what causes them.</p><p>Thanks for any help</p>]]></content>
			<author>
				<name><![CDATA[caswal]]></name>