	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Extruding vs Printing Temperature]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/6281/" />
	<updated>2014-04-28T16:16:29Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/6281/extruding-vs-printing-temperature/</id>
		<entry>
			<title type="html"><![CDATA[Re: Extruding vs Printing Temperature]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55234/#p55234" />
			<content type="html"><![CDATA[<p>I may be off on this.&nbsp; I get dark spots on my prints sometimes too.&nbsp; It&#039;s kind of frustrating.&nbsp; I think mine come from residue on the outside of the nozzle from where I had a failed print and the head plowed through some plastic.&nbsp; It&#039; seems to help if I clean it up some.</p>]]></content>
			<author>
				<name><![CDATA[bbriggsgeek]]></name>
				<uri>https://www.soliforum.com/user/2428/</uri>
			</author>
			<updated>2014-04-28T16:16:29Z</updated>
			<id>https://www.soliforum.com/post/55234/#p55234</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Extruding vs Printing Temperature]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55170/#p55170" />
			<content type="html"><![CDATA[<p>Hi Tim!<br />This is the one that I am usnig: LG HF380 - Melt Temperature (210~240) / Melt Flow Rate (43). Using a 0.35mm RepRap nozzle to extrude 3mm filament.</p>]]></content>
			<author>
				<name><![CDATA[henriquesv]]></name>
				<uri>https://www.soliforum.com/user/3986/</uri>
			</author>
			<updated>2014-04-27T11:33:14Z</updated>
			<id>https://www.soliforum.com/post/55170/#p55170</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Extruding vs Printing Temperature]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55141/#p55141" />
			<content type="html"><![CDATA[<p>Really too many variables to say here. We don&#039;t know what ABS resin you&#039;re using, or what hot end you&#039;re using. Finding ideal printing temperature is a bit of trial and error.</p><p>I extrude MG94 ABS at 187C, and print it at 205C on a Solidoodle hot end.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2014-04-26T16:10:31Z</updated>
			<id>https://www.soliforum.com/post/55141/#p55141</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Extruding vs Printing Temperature]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55134/#p55134" />
			<content type="html"><![CDATA[<p>Hi!<br />I&#039;ve been extruding ABS for some time already. For the ABS that I am using I set extrusion to 180ºC. But I still didn&#039;t get the proper temperature for 3D Printing. Have you guys reached any relation between extruding and printing?</p><p>For instance, while printing at 215ºC the melt flow seems right, but once in a while I get burned spots.</p><p>Any ideas on this one?</p><p>Thanks!</p>]]></content>
			<author>
				<name><![CDATA[henriquesv]]></name>
				<uri>https://www.soliforum.com/user/3986/</uri>
			</author>
			<updated>2014-04-26T12:49:16Z</updated>
			<id>https://www.soliforum.com/post/55134/#p55134</id>
		</entry>