		<entry>
			<title type="html"><![CDATA[Re: Snowflake Cookie Cutter]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/6383/#p6383" />
			<content type="html"><![CDATA[<p>Ian, any chance we can get your KISS slicer config in a nice downloadable ini?</p>]]></content>
			<author>
				<name><![CDATA[ErroneousBosch]]></name>
				<uri>https://www.soliforum.com/user/35/</uri>
			</author>
			<updated>2012-12-05T16:55:31Z</updated>
			<id>https://www.soliforum.com/post/6383/#p6383</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Snowflake Cookie Cutter]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5475/#p5475" />
			<content type="html"><![CDATA[<p>I designed and printed a snowflake cookie cutter too, but mine doesn&#039;t look like yours.&nbsp; Guess it&#039;s true what they say...&nbsp; &nbsp;Nice job Ian.</p>]]></content>
			<author>
				<name><![CDATA[cmetzel]]></name>
				<uri>https://www.soliforum.com/user/78/</uri>
			</author>
			<updated>2012-11-23T20:23:37Z</updated>
			<id>https://www.soliforum.com/post/5475/#p5475</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Snowflake Cookie Cutter]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5469/#p5469" />
			<content type="html"><![CDATA[<p>Going to print this when I get home.</p>]]></content>
			<author>
				<name><![CDATA[Brad]]></name>
				<uri>https://www.soliforum.com/user/2/</uri>
			</author>
			<updated>2012-11-23T18:39:54Z</updated>
			<id>https://www.soliforum.com/post/5469/#p5469</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Snowflake Cookie Cutter]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5459/#p5459" />
			<content type="html"><![CDATA[<p>The base is about 95mm.&nbsp; It was kapton with a bit of hairspray in a closed case, so it was pretty good.&nbsp; Also the base is mostly an open ring so there aren&#039;t many places where the force from shrinkage can reach all the way across the print.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2012-11-23T17:23:15Z</updated>
			<id>https://www.soliforum.com/post/5459/#p5459</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Snowflake Cookie Cutter]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5458/#p5458" />
			<content type="html"><![CDATA[<p>Very nice Ian!&nbsp; </p><p>I&#039;m surprised the base didn&#039;t warp, its quite large and flat. My first guess was you printed in PLA, but then mentioned acetone smoothing so it must be ABS.</p>]]></content>
			<author>
				<name><![CDATA[3Dprintergear]]></name>
				<uri>https://www.soliforum.com/user/80/</uri>
			</author>
			<updated>2012-11-23T17:19:56Z</updated>
			<id>https://www.soliforum.com/post/5458/#p5458</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Snowflake Cookie Cutter]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/5456/#p5456" />
			<content type="html"><![CDATA[<p><span class="postimg"><img src="http://solidoodletips.files.wordpress.com/2012/11/img_3157.jpg" alt="http://solidoodletips.files.wordpress.com/2012/11/img_3157.jpg" /></span></p><p><a href="http://www.thingiverse.com/thing:35442">http://www.thingiverse.com/thing:35442</a></p><p>It didn&#039;t slice very well in Slic3r 096, so I recommend Skeinforge or KISSlicer for this one.&nbsp; Set the extrusion width to .35mm so the wall prints as 2 perimeters.&nbsp; I recommend acetone smoothing to add strength, especially to keep the edge from splitting.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2012-11-23T16:46:13Z</updated>
			<id>https://www.soliforum.com/post/5456/#p5456</id>
		</entry>