<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Slicer question/request]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/6138/" />
	<updated>2014-04-13T22:32:09Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/6138/slicer-questionrequest/</id>
		<entry>
			<title type="html"><![CDATA[Re: Slicer question/request]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/54146/#p54146" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>pcm81 wrote:</cite><blockquote><p>Hello all,<br />I ran into an interesting issue with Slicer, well with 3d printing using slicer to be exact. When I print with nylon, i use brim and i am on mirror plate + Hairspray. My parts do curl and they pull hard enough that the brim rips off the part. The brim is still attached&nbsp; to print bed, but the part&#039;s corner is no longer attached&nbsp; to the brim. Is there any way to add layer thickness to the brim section, just like there is the skirt height parameter. I think if i made brim about 1mm thick it would work wonderfully.</p></blockquote></div><p>You could just add it into the design.&nbsp; I know of no way to make brim with more than one layer.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-04-13T22:32:09Z</updated>
			<id>https://www.soliforum.com/post/54146/#p54146</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Slicer question/request]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/54131/#p54131" />
			<content type="html"><![CDATA[<p>Hello all,<br />I ran into an interesting issue with Slicer, well with 3d printing using slicer to be exact. When I print with nylon, i use brim and i am on mirror plate + Hairspray. My parts do curl and they pull hard enough that the brim rips off the part. The brim is still attached&nbsp; to print bed, but the part&#039;s corner is no longer attached&nbsp; to the brim. Is there any way to add layer thickness to the brim section, just like there is the skirt height parameter. I think if i made brim about 1mm thick it would work wonderfully.</p>]]></content>
			<author>
				<name><![CDATA[pcm81]]></name>
				<uri>https://www.soliforum.com/user/1923/</uri>
			</author>
			<updated>2014-04-13T15:52:38Z</updated>
			<id>https://www.soliforum.com/post/54131/#p54131</id>
		</entry>
</feed>