	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Temps settings for extruding OSP from printer]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/5957/" />
	<updated>2014-03-25T16:18:18Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/5957/temps-settings-for-extruding-osp-from-printer/</id>
		<entry>
			<title type="html"><![CDATA[Re: Temps settings for extruding OSP from printer]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52927/#p52927" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>techbuilder2175 wrote:</cite><blockquote><div class="quotebox"><cite>insta wrote:</cite><blockquote><p>I print at 230C without issues, besides clogs (something something melt filter).</p></blockquote></div><p>Do you not use a melt filter?</p></blockquote></div><p>Not yet, I have two on the bench, but I&#039;m currently purging before I install them.</p>]]></content>
			<author>
				<name><![CDATA[insta]]></name>
				<uri>https://www.soliforum.com/user/5215/</uri>
			</author>
			<updated>2014-03-25T16:18:18Z</updated>
			<id>https://www.soliforum.com/post/52927/#p52927</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temps settings for extruding OSP from printer]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52885/#p52885" />
			<content type="html"><![CDATA[<p>I thought so but I was just checking since ysb mentioned he was printing OSP filament at 175 to 180 <br />which is 205 to 210 and I thought that was a little low so I just wanted to verify&nbsp; </p><p><a href="http://www.soliforum.com/topic/2469/finally-i-can-print-with-filastruder-filament-without-clog-my-extruder/">http://www.soliforum.com/topic/2469/fin … -extruder/</a></p>]]></content>
			<author>
				<name><![CDATA[techbuilder2175]]></name>
				<uri>https://www.soliforum.com/user/2779/</uri>
			</author>
			<updated>2014-03-25T07:49:54Z</updated>
			<id>https://www.soliforum.com/post/52885/#p52885</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temps settings for extruding OSP from printer]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52879/#p52879" />
			<content type="html"><![CDATA[<p>230C on most printers, 200C on Solidoodles. Just like most ABS out there. <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2014-03-25T05:16:21Z</updated>
			<id>https://www.soliforum.com/post/52879/#p52879</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temps settings for extruding OSP from printer]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52856/#p52856" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>insta wrote:</cite><blockquote><p>I print at 230C without issues, besides clogs (something something melt filter).</p></blockquote></div><p>Do you not use a melt filter?</p>]]></content>
			<author>
				<name><![CDATA[techbuilder2175]]></name>
				<uri>https://www.soliforum.com/user/2779/</uri>
			</author>
			<updated>2014-03-24T23:12:07Z</updated>
			<id>https://www.soliforum.com/post/52856/#p52856</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Temps settings for extruding OSP from printer]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52853/#p52853" />
			<content type="html"><![CDATA[<p>I print at 230C without issues, besides clogs (something something melt filter).</p>]]></content>
			<author>
				<name><![CDATA[insta]]></name>
				<uri>https://www.soliforum.com/user/5215/</uri>
			</author>
			<updated>2014-03-24T22:27:13Z</updated>
			<id>https://www.soliforum.com/post/52853/#p52853</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Temps settings for extruding OSP from printer]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52842/#p52842" />
			<content type="html"><![CDATA[<p>Hi everyone,</p><p>I just wanted to know what print temps your running with <br />when using filastruder filament using OSP pellets?</p><p>Reason I&#039;m asking is I&#039;m going to purchase a temp mod for my Afinia and I want to get an idea <br />as to what temps I need before I purchase the item.</p>]]></content>
			<author>
				<name><![CDATA[techbuilder2175]]></name>
				<uri>https://www.soliforum.com/user/2779/</uri>
			</author>
			<updated>2014-03-24T21:32:10Z</updated>
			<id>https://www.soliforum.com/post/52842/#p52842</id>
		</entry>