			<content type="html"><![CDATA[<p>After completing my mods I tried making a shaft coupler out of aluminum.&nbsp; Let&#039;s just say that I and tools are not best of friends but TurboCad and I are.&nbsp; So, here is my version of solid coupler.</p>]]></content>