			<title type="html"><![CDATA[Re: Extrusion calibration]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48226/#p48226" />
			<content type="html"><![CDATA[<p>Here you go watch the video in the calibration link ---&gt; <a href="http://www.soliwiki.com/Main_Page#Calibrations">http://www.soliwiki.com/Main_Page#Calibrations</a> Ian show you several ways to program it to the correct number.</p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2014-01-30T07:00:35Z</updated>
			<id>https://www.soliforum.com/post/48226/#p48226</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Extrusion calibration]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48220/#p48220" />
			<content type="html"><![CDATA[<p>I am just a little confused about how to calibrate my extrude. It is obviouly extruding too much and I need to pull it back a bit. I am working with a solid doodle 2 pro, Repitier, and sli3r.</p><p>And guidance?</p>]]></content>
			<author>
				<name><![CDATA[esterpa]]></name>
				<uri>https://www.soliforum.com/user/4441/</uri>
			</author>
			<updated>2014-01-30T05:17:55Z</updated>
			<id>https://www.soliforum.com/post/48220/#p48220</id>
		</entry>
</feed>