<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Support Material sticking too well to part]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/5345/" />
	<updated>2014-02-04T06:49:36Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/5345/support-material-sticking-too-well-to-part/</id>
		<entry>
			<title type="html"><![CDATA[Re: Support Material sticking too well to part]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48610/#p48610" />
			<content type="html"><![CDATA[<p>i love meshmixer. not often worth the effort tho <img src="https://www.soliforum.com/img/smilies/tongue.png" width="15" height="15" alt="tongue" />. oc ocassion, brilliant</p>]]></content>
			<author>
				<name><![CDATA[Tomek]]></name>
				<uri>https://www.soliforum.com/user/192/</uri>
			</author>
			<updated>2014-02-04T06:49:36Z</updated>
			<id>https://www.soliforum.com/post/48610/#p48610</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Support Material sticking too well to part]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48594/#p48594" />
			<content type="html"><![CDATA[<p>You could always try Kisslicer</p>]]></content>
			<author>
				<name><![CDATA[DePartedPrinter]]></name>
				<uri>https://www.soliforum.com/user/55/</uri>
			</author>
			<updated>2014-02-03T23:10:57Z</updated>
			<id>https://www.soliforum.com/post/48594/#p48594</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Support Material sticking too well to part]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48573/#p48573" />
			<content type="html"><![CDATA[<p>One huge discovery I have made recently is to generate support targeted material in the model instead of relying on the slicer... The slicer ALWAYS makes a mess of the print and requires a lot of clean up after printing. </p><p>Depending on the geometry of your print, this guide can be a huge help to support your model and requires a LOT less cleanup afterwards. Give it a shot. Once you do it one or twice it is pretty easy to do. </p><p><a href="http://www.extrudable.me/2013/12/28/meshmixer-2-0-best-newcomer-in-a-supporting-role/">http://www.extrudable.me/2013/12/28/mes … ting-role/</a></p>]]></content>
			<author>
				<name><![CDATA[downeym]]></name>
				<uri>https://www.soliforum.com/user/1737/</uri>
			</author>
			<updated>2014-02-03T20:14:59Z</updated>
			<id>https://www.soliforum.com/post/48573/#p48573</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Support Material sticking too well to part]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48110/#p48110" />
			<content type="html"><![CDATA[<p>...more settings pictures</p>]]></content>
			<author>
				<name><![CDATA[devsidell]]></name>
				<uri>https://www.soliforum.com/user/4000/</uri>
			</author>
			<updated>2014-01-29T16:43:43Z</updated>
			<id>https://www.soliforum.com/post/48110/#p48110</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Support Material sticking too well to part]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48109/#p48109" />
			<content type="html"><![CDATA[<p>***UPDATE***</p><p>I changed some more settings with Slic3r in RH and now the support material is breaking off in one nice piece.&nbsp; I&#039;ve uploaded pictures of my setting below.&nbsp; This is for my Solidoodle 3.&nbsp; ABS is extruding from 210C .35mm Nozzle and the print bed is at 110C.</p>]]></content>
			<author>
				<name><![CDATA[devsidell]]></name>
				<uri>https://www.soliforum.com/user/4000/</uri>
			</author>
			<updated>2014-01-29T16:42:32Z</updated>
			<id>https://www.soliforum.com/post/48109/#p48109</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Support Material sticking too well to part]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48099/#p48099" />
			<content type="html"><![CDATA[<p>no i havent.&nbsp; can&#039;t i just change the flow rate?</p>]]></content>
			<author>
				<name><![CDATA[devsidell]]></name>
				<uri>https://www.soliforum.com/user/4000/</uri>
			</author>
			<updated>2014-01-29T15:28:37Z</updated>
			<id>https://www.soliforum.com/post/48099/#p48099</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Support Material sticking too well to part]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48056/#p48056" />
			<content type="html"><![CDATA[<p>If your printer is still overextruding then support material will have a better bond to the actual print... have you done any of the calibrations to fix the factory overextruding issues?</p><p><a href="http://www.soliwiki.com/Main_Page#Calibrations">http://www.soliwiki.com/Main_Page#Calibrations</a></p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2014-01-29T01:44:14Z</updated>
			<id>https://www.soliforum.com/post/48056/#p48056</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Support Material sticking too well to part]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/48041/#p48041" />
			<content type="html"><![CDATA[<p>I have this issue where the part prints and sticks to the bed just fine but the removal of the support material is almost impossible.&nbsp; Any advice?</p>]]></content>
			<author>
				<name><![CDATA[devsidell]]></name>
				<uri>https://www.soliforum.com/user/4000/</uri>
			</author>
			<updated>2014-01-28T22:39:07Z</updated>
			<id>https://www.soliforum.com/post/48041/#p48041</id>
		</entry>
</feed>