<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Unable to mix ABS slurry, it sits like oil on water.]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/5277/" />
	<updated>2014-01-23T17:21:04Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/5277/unable-to-mix-abs-slurry-it-sits-like-oil-on-water/</id>
		<entry>
			<title type="html"><![CDATA[Re: Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47529/#p47529" />
			<content type="html"><![CDATA[<p>i reckon on the &quot;acetone&quot; ... had some myself of ebay, was not 99.7% pure or whatever they advertised... reckoned it was diluted with water.. didnt have the same smell as my normal supply of acetone either... opened a case with ebay, guy accepted them for a cash return... got some elsewhere.. no probs!... i got the deal where it was buy 2 litres get one litre free.... everything that glitters is not always gold.... or acetone in my case!!</p>]]></content>
			<author>
				<name><![CDATA[saymo606]]></name>
				<uri>https://www.soliforum.com/user/456/</uri>
			</author>
			<updated>2014-01-23T17:21:04Z</updated>
			<id>https://www.soliforum.com/post/47529/#p47529</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47480/#p47480" />
			<content type="html"><![CDATA[<p>If it is colored, then the plastic used as a carrier for the pigment may be something other than ABS.&nbsp; If you have any natural (off white) ABS it might work better.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2014-01-23T04:10:35Z</updated>
			<id>https://www.soliforum.com/post/47480/#p47480</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47448/#p47448" />
			<content type="html"><![CDATA[<p>It might be the ABS.&nbsp; It&#039;s a white ABS I just recently got.&nbsp; Prints very well... but probably not 100% ABS.</p>]]></content>
			<author>
				<name><![CDATA[user64x]]></name>
				<uri>https://www.soliforum.com/user/4455/</uri>
			</author>
			<updated>2014-01-22T22:29:23Z</updated>
			<id>https://www.soliforum.com/post/47448/#p47448</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47444/#p47444" />
			<content type="html"><![CDATA[<p>My jar may be the gateway to another dimension...</p>]]></content>
			<author>
				<name><![CDATA[user64x]]></name>
				<uri>https://www.soliforum.com/user/4455/</uri>
			</author>
			<updated>2014-01-22T22:19:16Z</updated>
			<id>https://www.soliforum.com/post/47444/#p47444</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47443/#p47443" />
			<content type="html"><![CDATA[<p>You sure its plain ABS your are trying to dissolve, and that its actually acetone?</p><p>It&#039;s not a trick that causes Acetone to dissolve the chains in ABS to break it down... so if its not working, then either; its not &#039;plain&#039; ABS (is a co-polymer filament of some description); or its adulterated acetone (or not acetone at all); Or the basis of chemistry is somehow different inside the jar..... <img src="https://www.soliforum.com/img/smilies/wink.png" width="15" height="15" alt="wink" /></p>]]></content>
			<author>
				<name><![CDATA[adrian]]></name>
				<uri>https://www.soliforum.com/user/663/</uri>
			</author>
			<updated>2014-01-22T22:16:11Z</updated>
			<id>https://www.soliforum.com/post/47443/#p47443</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47442/#p47442" />
			<content type="html"><![CDATA[<p>I have a lid.&nbsp; The jar should be air tight.</p>]]></content>
			<author>
				<name><![CDATA[user64x]]></name>
				<uri>https://www.soliforum.com/user/4455/</uri>
			</author>
			<updated>2014-01-22T22:13:05Z</updated>
			<id>https://www.soliforum.com/post/47442/#p47442</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47438/#p47438" />
			<content type="html"><![CDATA[<p>place a lid on it, but if you are in a cyclical temperature area, or even just by the window, it would be wise to put a small pinprick hole on the top to prevent pressure buildup while not very meaningfully increasing acetone evaporation. That said I have one jar in my closet that does not have a pinprick; it&#039;s not the end of the world eitherway.</p>]]></content>
			<author>
				<name><![CDATA[Tomek]]></name>
				<uri>https://www.soliforum.com/user/192/</uri>
			</author>
			<updated>2014-01-22T22:01:55Z</updated>
			<id>https://www.soliforum.com/post/47438/#p47438</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47420/#p47420" />
			<content type="html"><![CDATA[<p>Did you have the lid on the jar?&nbsp; It looks to me like your acetone has evaporated enough to replace itself with water.&nbsp; So now you have a stinky jar of water.&nbsp; You don&#039;t need that much acetone just enough to cover the plastic in the jar.&nbsp; You also don&#039;t need to put it in hot water.&nbsp; Now that I think about it you don&#039;t need any of this just get your printer set up correctly and you won&#039;t have to use a slurry to make your prints.&nbsp; Now if your using this to fix prints that&#039;s another thing.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-01-22T20:11:22Z</updated>
			<id>https://www.soliforum.com/post/47420/#p47420</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Unable to mix ABS slurry, it sits like oil on water.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47418/#p47418" />
			<content type="html"><![CDATA[<p>So I took about 300mm of white ABS filament and put it into this glass jar filled with 1/3 full of acetone.&nbsp; Put the jar in hot water for a day.&nbsp; All of the filament dissolved and just a goop right now.&nbsp; But it won&#039;t mix with acetone.</p><p>The ABS goop and acetone just sit there in 2 layers in that jar.</p><p>I poked the goop and it&#039;s like tooth paste.&nbsp; Acetone that sit on top is very clear.</p>]]></content>
			<author>
				<name><![CDATA[user64x]]></name>
				<uri>https://www.soliforum.com/user/4455/</uri>
			</author>
			<updated>2014-01-22T19:58:37Z</updated>
			<id>https://www.soliforum.com/post/47418/#p47418</id>
		</entry>
</feed>