<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Need Help With Bulldog Extrusion Settings.]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/5245/" />
	<updated>2014-01-20T21:41:15Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/5245/need-help-with-bulldog-extrusion-settings/</id>
		<entry>
			<title type="html"><![CDATA[Re: Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47264/#p47264" />
			<content type="html"><![CDATA[<p>Congratulations!!! Post a Picture</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-01-20T21:41:15Z</updated>
			<id>https://www.soliforum.com/post/47264/#p47264</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47263/#p47263" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>wardjr wrote:</cite><blockquote><p>Your Welcome,<br />as far as the Z you might be able to put the screw in from the bottom side.&nbsp; That is how mine is.</p></blockquote></div><p>Got it printed well enough to install it.. now I have the glass bed, will probably print another Z extension after I calibrate it more..</p><p>I HAVE TO SAY WOW!! There is like absolutely no banding!! This set up is amazing!!</p>]]></content>
			<author>
				<name><![CDATA[Hyper_Cube]]></name>
				<uri>https://www.soliforum.com/user/4544/</uri>
			</author>
			<updated>2014-01-20T21:34:04Z</updated>
			<id>https://www.soliforum.com/post/47263/#p47263</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47256/#p47256" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>Hyper_Cube wrote:</cite><blockquote><div class="quotebox"><cite>wardjr wrote:</cite><blockquote><p>No bother at all.&nbsp; That&#039;s exactly right mines at about 485.&nbsp; You can just change it in EEPROM steps/mm E:</p></blockquote></div><p>Mine is at 570. Seems to be pretty spot on. Might need to fudge it a little. The one thing I wish I did before all this was print the Z-Stop extension so I could use my glass bed. Trying this now.</p><p>I can already tell this is going to better than my last setup. Although my prints aren&#039;t sticking to the Kapton.. the layers look pretty amazing!! Thanks for all the advice!! You are awesome! We are learning so much over here!</p></blockquote></div><p>Your Welcome,<br />as far as the Z you might be able to put the screw in from the bottom side.&nbsp; That is how mine is.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-01-20T20:37:38Z</updated>
			<id>https://www.soliforum.com/post/47256/#p47256</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47253/#p47253" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>wardjr wrote:</cite><blockquote><p>No bother at all.&nbsp; That&#039;s exactly right mines at about 485.&nbsp; You can just change it in EEPROM steps/mm E:</p></blockquote></div><p>Mine is at 570. Seems to be pretty spot on. Might need to fudge it a little. The one thing I wish I did before all this was print the Z-Stop extension so I could use my glass bed. Trying this now.</p><p>I can already tell this is going to better than my last setup. Although my prints aren&#039;t sticking to the Kapton.. the layers look pretty amazing!! Thanks for all the advice!! You are awesome! We are learning so much over here!</p>]]></content>
			<author>
				<name><![CDATA[Hyper_Cube]]></name>
				<uri>https://www.soliforum.com/user/4544/</uri>
			</author>
			<updated>2014-01-20T19:04:46Z</updated>
			<id>https://www.soliforum.com/post/47253/#p47253</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47245/#p47245" />
			<content type="html"><![CDATA[<p>No bother at all.&nbsp; That&#039;s exactly right mines at about 485.&nbsp; You can just change it in EEPROM steps/mm E:</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-01-20T18:18:46Z</updated>
			<id>https://www.soliforum.com/post/47245/#p47245</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47244/#p47244" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>wardjr wrote:</cite><blockquote><p>The bulldog XL is geared 5:1 so basically your steps per mm should be close to five times the original settings.</p></blockquote></div><p>Thanks, so I just need to change the E step/mm on the firmware then callibrate? Sorry to be such a bother. I&#039;m still trying to figure out what I&#039;m doing.</p>]]></content>
			<author>
				<name><![CDATA[Hyper_Cube]]></name>
				<uri>https://www.soliforum.com/user/4544/</uri>
			</author>
			<updated>2014-01-20T18:01:34Z</updated>
			<id>https://www.soliforum.com/post/47244/#p47244</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47231/#p47231" />
			<content type="html"><![CDATA[<p>The bulldog XL is geared 5:1 so basically your steps per mm should be close to five times the original settings.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-01-20T15:14:18Z</updated>
			<id>https://www.soliforum.com/post/47231/#p47231</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47230/#p47230" />
			<content type="html"><![CDATA[<p>The same extruder calibration as the stock parts</p><p>---&gt; <a href="http://www.soliwiki.com/Main_Page#Calibrations">http://www.soliwiki.com/Main_Page#Calibrations</a></p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2014-01-20T15:04:28Z</updated>
			<id>https://www.soliforum.com/post/47230/#p47230</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Need Help With Bulldog Extrusion Settings.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/47213/#p47213" />
			<content type="html"><![CDATA[<p>Finished installing my Bulldog and E3D an hour or two ago. Everything is hooked up correctly. </p><p>The issue I&#039;m having is the amount of filament coming out of the hotend isn&#039;t as much as it was with the stock parts. Not sure what settings I need to change to calibrate for the bulldog. Any help is appreciated.</p>]]></content>
			<author>
				<name><![CDATA[Hyper_Cube]]></name>
				<uri>https://www.soliforum.com/user/4544/</uri>
			</author>
			<updated>2014-01-20T07:42:05Z</updated>
			<id>https://www.soliforum.com/post/47213/#p47213</id>
		</entry>
</feed>