			<title type="html"><![CDATA[Re: Layer banding - Z Axis Anti-Backlash]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41685/#p41685" />
			<content type="html"><![CDATA[<p>Got the new nut is place together with the two new printed parts. Conclusion: no improvement what so ever. <br />Hmm, wonder what to try next? Any thoughts anybody??</p><p>Stein</p>]]></content>
			<author>
				<name><![CDATA[stein.inge]]></name>
				<uri>https://www.soliforum.com/user/3871/</uri>
			</author>
			<updated>2013-11-15T11:42:46Z</updated>
			<id>https://www.soliforum.com/post/41685/#p41685</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Layer banding - Z Axis Anti-Backlash]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41680/#p41680" />
			<content type="html"><![CDATA[<p>Ahhh, of course - got it :-) Thank&#039;s a lot elmoret.</p><br /><p>Regards Stein</p>]]></content>
			<author>
				<name><![CDATA[stein.inge]]></name>
				<uri>https://www.soliforum.com/user/3871/</uri>
			</author>
			<updated>2013-11-15T07:47:59Z</updated>
			<id>https://www.soliforum.com/post/41680/#p41680</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Layer banding - Z Axis Anti-Backlash]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41679/#p41679" />
			<content type="html"><![CDATA[<p>That nut you see has been added as part of the modification. Which is why it says:</p><div class="codebox"><pre><code>Supplies Needed:

Standard 5/16-18 Hex Nut
The (2) Printed Parts</code></pre></div><p>and</p><div class="codebox"><pre><code>Try your 5/16-18 Nut into the Inner to assuring it fits snug when it bottoms out.</code></pre></div>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2013-11-15T07:20:00Z</updated>
			<id>https://www.soliforum.com/post/41679/#p41679</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Layer banding - Z Axis Anti-Backlash]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41677/#p41677" />
			<content type="html"><![CDATA[<p>Hi 3D-oolder</p><p>That was actually my printer. I have since then removed as much of the rust as possible and greased it up.</p><p>Regards Stein</p>]]></content>
			<author>
				<name><![CDATA[stein.inge]]></name>
				<uri>https://www.soliforum.com/user/3871/</uri>
			</author>
			<updated>2013-11-15T07:02:40Z</updated>
			<id>https://www.soliforum.com/post/41677/#p41677</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Layer banding - Z Axis Anti-Backlash]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41676/#p41676" />
			<content type="html"><![CDATA[<p>Looks like you have a lot of rust.&nbsp; Before you do anything you might want to address that.</p><p>See this thread:<br /><a href="http://www.soliforum.com/topic/3781/my-printer-is-rusty/">http://www.soliforum.com/topic/3781/my- … -is-rusty/</a></p>]]></content>
			<author>
				<name><![CDATA[3d-oodler]]></name>
				<uri>https://www.soliforum.com/user/815/</uri>
			</author>
			<updated>2013-11-15T06:44:36Z</updated>
			<id>https://www.soliforum.com/post/41676/#p41676</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Layer banding - Z Axis Anti-Backlash]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41674/#p41674" />
			<content type="html"><![CDATA[<p>Hi folks<br />I see there is a good wiki on how to print to parts to prevent layer banding (Z Axis Anti-Backlash). In the wiki, the first picture shows a large hex nut on the threaded rod surrounded by four smaller nuts.</p><p>When I look at my printer, the setup is not the same. The large hex-nut is hidden in a layer of plywood. What should I do?</p><p>Should I rearrange my printer to look like the setup in the wiki and then add the two printed pieces as shown? Alternatively, should I just leave my printer as it is?</p><p>See the two attached pictures.</p>]]></content>
			<author>
				<name><![CDATA[stein.inge]]></name>
				<uri>https://www.soliforum.com/user/3871/</uri>
			</author>
			<updated>2013-11-15T06:31:12Z</updated>
			<id>https://www.soliforum.com/post/41674/#p41674</id>
		</entry>
</feed>